daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Ocean Mining: A Fluidic Electrochemical Route for Lithium Extraction from Seawater AITranslate

Singapore University of Technology and Design; Singapore University of Technology and Design; Singapore University of Technology and Design; Singapore University of Technology and Design; Singapore University of Technology and Design; Singapore University of Technology and Design; Singapore University of Technology and Design
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Mining lithium from the ocean has long been impeded by the lack of suitable lithium extracting technology. So far, adsorption and electrochemical strategies have been investigated. However, application of the adsorption method was limited by low adsorption rate and dissolution of adsorbent. In addition, experiments using the electrochemical method were either confined to lithium-enriched brine or performed in static electrochemical cell, which requires replacement of electrode. Herein, we report a fluidic electrochemical extraction (FEE) route for lithium extraction from seawater. This FEE system consists of an oxygen evolution cathode, a MnO2 working electrode, and an oxygen reduction anode. In operation, a voltage was applied on the cells to force Li+ to enter into MnO2 and release it as LiOH raw material. By virtue of the flow architecture, we have successfully extracted lithium from seawater with 7.0 ppm Li+. The highest absorption capacity reaches up to 20.6 mg Li+ per 1.0 g MnO2 for 0.8 h, corresponding to an electrical energy consumption of 7.2 Wh for extracting 1.0 g Li+. The fluidic electrochemical strategy developed in this study provides a remarkably effective method for lithium extraction from seawater and can be extended to extract other metal ions from the ocean or even in other fluids.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsmaterialslett.0c00385

Chinese Library Classification Number:

Citation Information:

Mining lithium from the ocean has long been impeded by the lack of suitable lithium extracting technology. So far, adsorption and electrochemical strategies have been investigated. However, application of the adsorption method was limited by low adsorption rate and dissolution of adsorbent. In addition, experiments using the electrochemical method were either confined to lithium-enriched brine or performed in static electrochemical cell, which requires replacement of electrode. Herein, we report a fluidic electrochemical extraction (FEE) route for lithium extraction from seawater. This FEE system consists of an oxygen evolution cathode, a MnO2 working electrode, and an oxygen reduction anode. In operation, a voltage was applied on the cells to force Li+ to enter into MnO2 and release it as LiOH raw material. By virtue of the flow architecture, we have successfully extracted lithium from seawater with 7.0 ppm Li+. The highest absorption capacity reaches up to 20.6 mg Li+ per 1.0 g MnO2 for 0.8 h, corresponding to an electrical energy consumption of 7.2 Wh for extracting 1.0 g Li+. The fluidic electrochemical strategy developed in this study provides a remarkably effective method for lithium extraction from seawater and can be extended to extract other metal ions from the ocean or even in other fluids.

quote

GB/T 7714-2015 [1] Juezhi Yu, Daliang Fang, Hang Zhang, et al. ACS Materials Letters, 2020(2). DOI:10.1021/acsmaterialslett.0c00385.
MLA [1] Juezhi Yu, et al., ACS Materials Letters, no. 2, 2020, https://doi.org/10.1021/acsmaterialslett.0c00385.
APA [1] Juezhi Yu, Daliang Fang, Hang Zhang, Zhi Yi Leong, Jingtao Zhang, Xiaoxia Li, & Hui Ying Yang. (2020). ACS Materials Letters(2). https://doi.org/10.1021/acsmaterialslett.0c00385
IEEE [1] Juezhi Yu, Daliang Fang, Hang Zhang, Zhi Yi Leong, Jingtao Zhang, Xiaoxia Li, and Hui Ying Yang, ACS Materials Letters, no. 2, 2020, doi: 10.1021/acsmaterialslett.0c00385.