Hydrogels Containing o-Nitrobenzyl Ester at Cross-Linking Points: Soft Matters for Fabrication of Functionalizable Microwells AITranslate

Gebze Technical University; Gebze Technical University; Gebze Technical University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Light-responsive o-nitrobenzyl ester-containing poly(ethylene glycol)-based hydrogel was synthesized via a nucleophilic Michael addition reaction, both as bulk gel and as a film on the glass surface. Obtained hydrogels were thoroughly characterized using Fourier transform infrared (FTIR) spectroscopy, thermogravimetric analysis (TGA), and scanning electron microscopy (SEM). Because of the presence of the photodegradable o-nitrobenzyl ester units, the hydrogels underwent degradation upon ultraviolet (UV) irradiation, yielding the amine-reactive nitrosobenzaldehyde groups at the newly formed interface. The photogenerated nitrosobenzaldehydes were further functionalized with amine-containing molecules, as proved by FTIR analysis. Additionally, the hydrogels were applied as films on glass surfaces, enabling patterned photodegradation by using photomasks with circular patterns. SEM analysis confirmed hydrogel etching and formation of microwells induced by UV irradiation. To assess the immobilization of bioactive ligands within the microwells, protein immobilization was performed. Fluorescence microscopy analysis demonstrated specific biofunctionalization exclusively within the microwells, while nonspecific adsorption was absent in the remaining parts of the hydrogel due to the antifouling nature of the PEG units. We believe that the reported hydrogel can be useful for applications that involve bioimmobilization.

KeyWords AITranslate

lightresponsive hydrogels photopatterning microwells onitrobenzyl ester aldehyde−amine coupling
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.3c02138

Chinese Library Classification Number:

Citation Information:

Light-responsive o-nitrobenzyl ester-containing poly(ethylene glycol)-based hydrogel was synthesized via a nucleophilic Michael addition reaction, both as bulk gel and as a film on the glass surface. Obtained hydrogels were thoroughly characterized using Fourier transform infrared (FTIR) spectroscopy, thermogravimetric analysis (TGA), and scanning electron microscopy (SEM). Because of the presence of the photodegradable o-nitrobenzyl ester units, the hydrogels underwent degradation upon ultraviolet (UV) irradiation, yielding the amine-reactive nitrosobenzaldehyde groups at the newly formed interface. The photogenerated nitrosobenzaldehydes were further functionalized with amine-containing molecules, as proved by FTIR analysis. Additionally, the hydrogels were applied as films on glass surfaces, enabling patterned photodegradation by using photomasks with circular patterns. SEM analysis confirmed hydrogel etching and formation of microwells induced by UV irradiation. To assess the immobilization of bioactive ligands within the microwells, protein immobilization was performed. Fluorescence microscopy analysis demonstrated specific biofunctionalization exclusively within the microwells, while nonspecific adsorption was absent in the remaining parts of the hydrogel due to the antifouling nature of the PEG units. We believe that the reported hydrogel can be useful for applications that involve bioimmobilization.

quote

GB/T 7714-2015 [1] Aleyna Turanli, Nisa Demirbilek, Tugce N. Gevrek. ACS Applied Polymer Materials, 2024(6). DOI:10.1021/acsapm.3c02138.
MLA [1] Aleyna Turanli, et al., ACS Applied Polymer Materials, no. 6, 2024, https://doi.org/10.1021/acsapm.3c02138.
APA [1] Aleyna Turanli, Nisa Demirbilek, & Tugce N. Gevrek. (2024). ACS Applied Polymer Materials(6). https://doi.org/10.1021/acsapm.3c02138
IEEE [1] Aleyna Turanli, Nisa Demirbilek, and Tugce N. Gevrek, ACS Applied Polymer Materials, no. 6, 2024, doi: 10.1021/acsapm.3c02138. keywords: {lightresponsive hydrogels;photopatterning;microwells;onitrobenzyl ester;aldehyde−amine coupling}