daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Self-Adhesive, Antifreezing, and Antidrying Conductive Glycerin/Polyacrylamide/Chitosan Quaternary Ammonium Salt Composite Hydrogel as a Flexible Strain Sensor AITranslate

Nanchang University; Nanchang University; Nanchang University; Nanchang University; Nanchang University; Nanchang University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Conductive hydrogels, a type of intrinsically flexible and conductive materials, are frequently employed in soft electronics. However, because water-based hydrogels can easily freeze and dry, their long-term stability is considerably limited. Herein, a glycerol (Gly)–water binary antifreezing and antidrying hydrogel was prepared by using glycine with water as a solvent, followed by the introduction of cationic polysaccharide chitosan quaternary ammonium salts into the covalently cross-linked polyacrylamide network and addition of NaCl ions to adjust the ionic conductivity of the hydrogel. In a broad temperature range, the produced hydrogel was used for tensile and sensitive strain sensing. Because strong hydrogen bonds between Gly and water molecules are easily established, the resultant organohydrogels have good freezing and drying endurance, retaining long-term deformation even at negative temperatures. Moreover, the hydrogel exhibits good adhesion and tensile properties because of the addition of chitosan quaternary ammonium salts. At the same time, strain sensors fabricated using the hydrogel exhibit a wide operating strain range (≈1000%) and good sensitivity, stability, and repeatability, making them promising candidates for building gel-based strain sensor platforms.

KeyWords AITranslate

antifreezing antidrying conductive hydrogel stretchable flexible sensing
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.3c02742

Chinese Library Classification Number:

Citation Information:

Conductive hydrogels, a type of intrinsically flexible and conductive materials, are frequently employed in soft electronics. However, because water-based hydrogels can easily freeze and dry, their long-term stability is considerably limited. Herein, a glycerol (Gly)–water binary antifreezing and antidrying hydrogel was prepared by using glycine with water as a solvent, followed by the introduction of cationic polysaccharide chitosan quaternary ammonium salts into the covalently cross-linked polyacrylamide network and addition of NaCl ions to adjust the ionic conductivity of the hydrogel. In a broad temperature range, the produced hydrogel was used for tensile and sensitive strain sensing. Because strong hydrogen bonds between Gly and water molecules are easily established, the resultant organohydrogels have good freezing and drying endurance, retaining long-term deformation even at negative temperatures. Moreover, the hydrogel exhibits good adhesion and tensile properties because of the addition of chitosan quaternary ammonium salts. At the same time, strain sensors fabricated using the hydrogel exhibit a wide operating strain range (≈1000%) and good sensitivity, stability, and repeatability, making them promising candidates for building gel-based strain sensor platforms.

quote

GB/T 7714-2015 [1] Song Liu, Li Wan, Feifan Hu, et al. ACS Applied Polymer Materials, 2024(6). DOI:10.1021/acsapm.3c02742.
MLA [1] Song Liu, et al., ACS Applied Polymer Materials, no. 6, 2024, https://doi.org/10.1021/acsapm.3c02742.
APA [1] Song Liu, Li Wan, Feifan Hu, Zhiwei Wen, Ming Cao, & Fanrong Ai. (2024). ACS Applied Polymer Materials(6). https://doi.org/10.1021/acsapm.3c02742
IEEE [1] Song Liu, Li Wan, Feifan Hu, Zhiwei Wen, Ming Cao, and Fanrong Ai, ACS Applied Polymer Materials, no. 6, 2024, doi: 10.1021/acsapm.3c02742. keywords: {antifreezing;antidrying;conductive hydrogel;stretchable;flexible sensing}