Abstract AITranslate

A combined ab initio and thermodynamic study of the Cu–Dy system has been performed and a self-consistent thermodynamic database has been obtained. Density functional theory has been applied by using the VASP code in order to obtain the enthalpy of formation at 0 K of intermetallic compounds. Experimental information on the Cu–Dy phase diagram and thermodynamic properties of its alloys have been collected. Using these data, optimized parameters have been obtained by applying the CALPHAD approach. The present results reproduce the experimental data available reasonably well, although some features of the Cu–Dy system need to be further clarified.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1016/j.calphad.2009.04.001

Chinese Library Classification Number:

Citation Information:

A combined ab initio and thermodynamic study of the Cu–Dy system has been performed and a self-consistent thermodynamic database has been obtained. Density functional theory has been applied by using the VASP code in order to obtain the enthalpy of formation at 0 K of intermetallic compounds. Experimental information on the Cu–Dy phase diagram and thermodynamic properties of its alloys have been collected. Using these data, optimized parameters have been obtained by applying the CALPHAD approach. The present results reproduce the experimental data available reasonably well, although some features of the Cu–Dy system need to be further clarified.

quote

GB/T 7714-2015 [1] M. Palumbo, L. Battezzati, A. Pasturel, et al. Calphad, 2009(33). DOI:10.1016/j.calphad.2009.04.001.
MLA [1] M. Palumbo, et al., Calphad, no. 33, 2009, https://doi.org/10.1016/j.calphad.2009.04.001.
APA [1] M. Palumbo, L. Battezzati, A. Pasturel, S. GottliebSchönmeyer, & W. Assmus. (2009). Calphad(33). https://doi.org/10.1016/j.calphad.2009.04.001
IEEE [1] M. Palumbo, L. Battezzati, A. Pasturel, S. GottliebSchönmeyer, and W. Assmus, Calphad, no. 33, 2009, doi: 10.1016/j.calphad.2009.04.001.