Computational modeling of elastic properties of carbon nanotube/polymer composites with interphase regions. Part II: Mechanical modeling AITranslate
Abstract AITranslate
Highlights • First critical comparison between local and hybrid local/non-local mechanics for prediction of effective properties of nano reinforced polymers. • Original conclusions about the effects of complex microstructures on the effective properties (clusters, interphases properties). • Insights about differences between local and hybrid models on local mechanical fields at the small scale. We present two modeling approaches for predicting the macroscopic elastic properties of carbon nanotubes/polymer composites with thick interphase regions at the nanotube/matrix frontier. The first model is based on local continuum mechanics; the second one is based on hybrid local/non-local continuum mechanics. The key computational issues, including the peculiar homogenization technique and treatment of periodical boundary conditions in the non-local continuum model, are clarified. Both models are implemented through a three-dimensional geometric representation of the carbon nanotubes network, which has been detailed in Part I. Numerical results are shown and compared for both models in order to test convergence and sensitivity toward input parameters. It is found that both approaches provide similar results in terms of homogenized quantities but locally can lead to very different microscopic fields.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1016/j.commatsci.2013.07.008
Chinese Library Classification Number:
Citation Information:
Highlights • First critical comparison between local and hybrid local/non-local mechanics for prediction of effective properties of nano reinforced polymers. • Original conclusions about the effects of complex microstructures on the effective properties (clusters, interphases properties). • Insights about differences between local and hybrid models on local mechanical fields at the small scale. We present two modeling approaches for predicting the macroscopic elastic properties of carbon nanotubes/polymer composites with thick interphase regions at the nanotube/matrix frontier. The first model is based on local continuum mechanics; the second one is based on hybrid local/non-local continuum mechanics. The key computational issues, including the peculiar homogenization technique and treatment of periodical boundary conditions in the non-local continuum model, are clarified. Both models are implemented through a three-dimensional geometric representation of the carbon nanotubes network, which has been detailed in Part I. Numerical results are shown and compared for both models in order to test convergence and sensitivity toward input parameters. It is found that both approaches provide similar results in terms of homogenized quantities but locally can lead to very different microscopic fields.
quote
| GB/T 7714-2015 | [1] Fei Han, Yan Azdoud, Gilles Lubineau. Computational Materials Science, 2014(81). DOI:10.1016/j.commatsci.2013.07.008. |
| MLA | [1] Fei Han, et al., Computational Materials Science, no. 81, 2014, https://doi.org/10.1016/j.commatsci.2013.07.008. |
| APA | [1] Fei Han, Yan Azdoud, & Gilles Lubineau. (2014). Computational Materials Science(81). https://doi.org/10.1016/j.commatsci.2013.07.008 |
| IEEE | [1] Fei Han, Yan Azdoud, and Gilles Lubineau, Computational Materials Science, no. 81, 2014, doi: 10.1016/j.commatsci.2013.07.008. |