daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

A Solvent-Free Photochemical Route to Clickable Multifunctional Polyacrylic Elastomers AITranslate

Sichuan University; Sichuan University; Sichuan University; Sichuan University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Multifunctional polyacrylic elastomers with ultrastrechability, hydrophobicity, self-healing, and adhesive properties have wide applications in wearable electronics, sensors, soft robotics, and biomedical science. However, it is challenging to integrate these functionalities into one material in a simple solvent-free approach. To address this challenge, we herein develop a two-step bulk photopolymerization method to make ultrastretchable, adhesive, self-healable, hydrophobicity-tunable elastomers by adding a small amount of 1-ethynylcyclohexyl acrylate (ECA) into a common acrylate, ethyl acrylate. ECA efficiently prevents uncontrollable solidification during the first step photopolymerization and acts as a cross-linker to make elastomers in the second step photocuring. When ECA increases from 0.5 to 3.3 mol %, the maximum strain of elastomers decreases from 3087 to 1763% and the maximum stress increases from 0.19 to 1.04 MPa. These elastomers show a peeling strength of 1233–1621 N/m when adhering to different surfaces, including glass, steel, and polymethyl mathacrylate . They can self-heal to its original modulus with a fracture strain of 1100% and fraction stress of 0.5 MPa. In addition, we can use surface photoclick thio-yne reactions to tune the hydrophobicity with contact angles from 113° ± 2° to 79° ± 2°. We believe that our environmental-friendly solvent-free approach toward multifunctional polyacrylate elastomers will expand their applications in various areas.

KeyWords AITranslate

photopolymerization acetylene acrylate polyacrylic elastomers photoclick reaction selfhealing adhesion
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.2c00833

Chinese Library Classification Number:

Citation Information:

Multifunctional polyacrylic elastomers with ultrastrechability, hydrophobicity, self-healing, and adhesive properties have wide applications in wearable electronics, sensors, soft robotics, and biomedical science. However, it is challenging to integrate these functionalities into one material in a simple solvent-free approach. To address this challenge, we herein develop a two-step bulk photopolymerization method to make ultrastretchable, adhesive, self-healable, hydrophobicity-tunable elastomers by adding a small amount of 1-ethynylcyclohexyl acrylate (ECA) into a common acrylate, ethyl acrylate. ECA efficiently prevents uncontrollable solidification during the first step photopolymerization and acts as a cross-linker to make elastomers in the second step photocuring. When ECA increases from 0.5 to 3.3 mol %, the maximum strain of elastomers decreases from 3087 to 1763% and the maximum stress increases from 0.19 to 1.04 MPa. These elastomers show a peeling strength of 1233–1621 N/m when adhering to different surfaces, including glass, steel, and polymethyl mathacrylate . They can self-heal to its original modulus with a fracture strain of 1100% and fraction stress of 0.5 MPa. In addition, we can use surface photoclick thio-yne reactions to tune the hydrophobicity with contact angles from 113° ± 2° to 79° ± 2°. We believe that our environmental-friendly solvent-free approach toward multifunctional polyacrylate elastomers will expand their applications in various areas.

quote

GB/T 7714-2015 [1] Hongyu Yan, Zhengyuan Zhang, Ming Xiao, et al. ACS Applied Polymer Materials, 2022(4). DOI:10.1021/acsapm.2c00833.
MLA [1] Hongyu Yan, et al., ACS Applied Polymer Materials, no. 4, 2022, https://doi.org/10.1021/acsapm.2c00833.
APA [1] Hongyu Yan, Zhengyuan Zhang, Ming Xiao, & Yuechuan Wang. (2022). ACS Applied Polymer Materials(4). https://doi.org/10.1021/acsapm.2c00833