Hybrid Tandem Quantum Dot/Organic Solar Cells with Enhanced Photocurrent and Efficiency via Ink and Interlayer Engineering AITranslate
Abstract AITranslate
Realization of colloidal quantum dot (CQD)/organic photovoltaic (OPV) tandem solar cells that integrate the strong infrared absorption of CQDs with large photovoltages of OPVs is an attractive option toward high-performing, low-cost thin-film solar cells. To date, monolithic hybrid tandem integration of CQD/OPV solar cells has been restricted due to the CQD ink’s catastrophic damage to the organic subcell, thus forcing the low-band-gap CQD to be used as a front cell. This suboptimal configuration limits the maximum achievable photocurrent in CQD/OPV hybrid tandem solar cells. In this work, we demonstrate hybrid tandem solar cells employing a low-band-gap CQD back cell on top of an organic front cell thanks to a modified CQD ink formulation and a robust interconnection layer (ICL), which together overcome the long-standing integration challenges for CQD and organic subcells. The resulting tandem architecture surpasses previously reported current densities by ∼20–25% and yields a state-of-the-art power conversion efficiency (PCE) of 9.4%.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsenergylett.8b00460
Chinese Library Classification Number:
Citation Information:
Realization of colloidal quantum dot (CQD)/organic photovoltaic (OPV) tandem solar cells that integrate the strong infrared absorption of CQDs with large photovoltages of OPVs is an attractive option toward high-performing, low-cost thin-film solar cells. To date, monolithic hybrid tandem integration of CQD/OPV solar cells has been restricted due to the CQD ink’s catastrophic damage to the organic subcell, thus forcing the low-band-gap CQD to be used as a front cell. This suboptimal configuration limits the maximum achievable photocurrent in CQD/OPV hybrid tandem solar cells. In this work, we demonstrate hybrid tandem solar cells employing a low-band-gap CQD back cell on top of an organic front cell thanks to a modified CQD ink formulation and a robust interconnection layer (ICL), which together overcome the long-standing integration challenges for CQD and organic subcells. The resulting tandem architecture surpasses previously reported current densities by ∼20–25% and yields a state-of-the-art power conversion efficiency (PCE) of 9.4%.
quote
| GB/T 7714-2015 | [1] Taesoo Kim, Yuliar Firdaus, Ahmad R. Kirmani, et al. ACS Energy Letters, 2018(3). DOI:10.1021/acsenergylett.8b00460. |
| MLA | [1] Taesoo Kim, et al., ACS Energy Letters, no. 3, 2018, https://doi.org/10.1021/acsenergylett.8b00460. |
| APA | [1] Taesoo Kim, Yuliar Firdaus, Ahmad R. Kirmani, RuZe Liang, Hanlin Hu, Mengxia Liu, Abdulrahman El Labban, Sjoerd Hoogland, Pierre M. Beaujuge, Edward H. Sargent, & Aram Amassian. (2018). ACS Energy Letters(3). https://doi.org/10.1021/acsenergylett.8b00460 |
| IEEE | [1] Taesoo Kim, Yuliar Firdaus, Ahmad R. Kirmani, RuZe Liang, Hanlin Hu, Mengxia Liu, Abdulrahman El Labban, Sjoerd Hoogland, Pierre M. Beaujuge, Edward H. Sargent, and Aram Amassian, ACS Energy Letters, no. 3, 2018, doi: 10.1021/acsenergylett.8b00460. |