daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

HDPE/EVOH Multilayered, High Barrier Films for Flexible Organic Photovoltaic Device Packaging AITranslate

Case Western Reserve University; Case Western Reserve University; Case Western Reserve University; Case Western Reserve University; Case Western Reserve University; Case Western Reserve University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Transparent films composed of 65 alternating layers of high density polyethylene and ethylene/vinyl alcohol copolymer were produced and evaluated for their oxygen and water vapor barrier performance. Such high barrier films are of special interest for encapsulation of flexible organic electronic devices; these devices are extraordinarily sensitive to degradation by oxygen and/or water. In the present work, the multilayered films were produced using a layer multiplying process, and in some cases, they were further modified by applying organic and inorganic barrier coatings. An optimized film included coatings of both parylene C and alumina, achieving an oxygen transmission rate of <10–3 cc/m2·day and a water vapor transition rate of 4.6 × 10–4 g/m2·day; these values are useful in encapsulating organic photovoltaic devices.

KeyWords AITranslate

barrier film layered coatings OLED parylene alumina
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.8b00181

Chinese Library Classification Number:

Citation Information:

Transparent films composed of 65 alternating layers of high density polyethylene and ethylene/vinyl alcohol copolymer were produced and evaluated for their oxygen and water vapor barrier performance. Such high barrier films are of special interest for encapsulation of flexible organic electronic devices; these devices are extraordinarily sensitive to degradation by oxygen and/or water. In the present work, the multilayered films were produced using a layer multiplying process, and in some cases, they were further modified by applying organic and inorganic barrier coatings. An optimized film included coatings of both parylene C and alumina, achieving an oxygen transmission rate of <10–3 cc/m2·day and a water vapor transition rate of 4.6 × 10–4 g/m2·day; these values are useful in encapsulating organic photovoltaic devices.

quote

GB/T 7714-2015 [1] Mingze Sun, Sunsheng Zhu, Ci Zhang, et al. ACS Applied Polymer Materials, 2019(1). DOI:10.1021/acsapm.8b00181.
MLA [1] Mingze Sun, et al., ACS Applied Polymer Materials, no. 1, 2019, https://doi.org/10.1021/acsapm.8b00181.
APA [1] Mingze Sun, Sunsheng Zhu, Ci Zhang, Andrew Olah, Eric Baer, & David A. Schiraldi. (2019). ACS Applied Polymer Materials(1). https://doi.org/10.1021/acsapm.8b00181
IEEE [1] Mingze Sun, Sunsheng Zhu, Ci Zhang, Andrew Olah, Eric Baer, and David A. Schiraldi, ACS Applied Polymer Materials, no. 1, 2019, doi: 10.1021/acsapm.8b00181. keywords: {barrier;film;layered;coatings;OLED;parylene;alumina}