Abstract AITranslate

The effects of I2 oxidation on the behavior of Cu2xS nanoparticles—their long-term localized-surface plasmon resonance (LSPR), crystal structure, composition, and ability to undergo cation exchange—were explored. I2 has been known to induce a blue shift in the LSPR of Cu2xS nanoparticles due to the increase in the hole concentration through the removal of Cu+ ions. An unexpected red shift is observed in I2-exposed Cu2–xS nanoparticles over the longer times required for cation exchange. Despite this complication of the LSPR behavior, the process of cation exchange from Cu+ to Cd2+ is modulated by the exposure of the Cu2xS nanoparticle precursor to elemental iodide, I2. This is consistent with the promotion of cation exchange through increased vacancy concentration. Treatment with I2 induces a greater extent of cation exchange than in controls. Increasing I2 exposure results in a greater extent of exchange and exchange at lower temperatures. The increased mobility of sulfide ions to which the red shift in LSPR is attributed also affects the resultant CdS crystal structure. Zinc-blende CdS, which has an altered anion network, is observed upon increased I2 exposure or extended cation-exchange reaction times. This work offers insights into the mechanism of cation exchange and the modulation of the LSPR of plasmonic semiconductors.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsmaterialslett.9b00402

Chinese Library Classification Number:

Citation Information:

The effects of I2 oxidation on the behavior of Cu2xS nanoparticles—their long-term localized-surface plasmon resonance (LSPR), crystal structure, composition, and ability to undergo cation exchange—were explored. I2 has been known to induce a blue shift in the LSPR of Cu2xS nanoparticles due to the increase in the hole concentration through the removal of Cu+ ions. An unexpected red shift is observed in I2-exposed Cu2–xS nanoparticles over the longer times required for cation exchange. Despite this complication of the LSPR behavior, the process of cation exchange from Cu+ to Cd2+ is modulated by the exposure of the Cu2xS nanoparticle precursor to elemental iodide, I2. This is consistent with the promotion of cation exchange through increased vacancy concentration. Treatment with I2 induces a greater extent of cation exchange than in controls. Increasing I2 exposure results in a greater extent of exchange and exchange at lower temperatures. The increased mobility of sulfide ions to which the red shift in LSPR is attributed also affects the resultant CdS crystal structure. Zinc-blende CdS, which has an altered anion network, is observed upon increased I2 exposure or extended cation-exchange reaction times. This work offers insights into the mechanism of cation exchange and the modulation of the LSPR of plasmonic semiconductors.

quote

GB/T 7714-2015 [1] Han K. D. Le, Huiyan Xiong, Bonnie A. Page, et al. ACS Materials Letters, 2020(2). DOI:10.1021/acsmaterialslett.9b00402.
MLA [1] Han K. D. Le, et al., ACS Materials Letters, no. 2, 2020, https://doi.org/10.1021/acsmaterialslett.9b00402.
APA [1] Han K. D. Le, Huiyan Xiong, Bonnie A. Page, Luis F. GarciaHerrera, Haley P. McAllister, Boxi Cameron Li, Haiying Wang, & Katherine E. Plass. (2020). ACS Materials Letters(2). https://doi.org/10.1021/acsmaterialslett.9b00402
IEEE [1] Han K. D. Le, Huiyan Xiong, Bonnie A. Page, Luis F. GarciaHerrera, Haley P. McAllister, Boxi Cameron Li, Haiying Wang, and Katherine E. Plass, ACS Materials Letters, no. 2, 2020, doi: 10.1021/acsmaterialslett.9b00402.