Frontal Polymerization in Short-Fiber-Reinforced Thermoset Composites AITranslate

University of Illinois; University of Illinois; University of Illinois
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Frontal polymerization (FP) has recently been introduced as a faster, more energy-efficient manufacturing process for high-performance thermoset composites. This numerical study focuses on the FP-based manufacturing of short-fiber-reinforced polymeric matrix composites. The investigation involves a combination of multiphysics finite element analyses and analytical predictions. The developed model is also applied to a short-fiber composite with spatially varying fiber orientation obtained from a sample produced by vacuum injection method. The results show how the steady-state front velocity and inclination angle depend on the fiber orientation angle and volume fraction. Analytical expressions are derived to capture that dependence and show excellent agreement with the numerical steady-state results. Simulations of FP in short-fiber composites based on experimental distributions of the fiber orientation indicate the feasibility of FP in samples prepared by injection molding.

KeyWords AITranslate

frontal polymerization shortfiberreinforced composite carbon fiber finite element analysis dicyclopentadiene
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.2c00818

Chinese Library Classification Number:

Citation Information:

Frontal polymerization (FP) has recently been introduced as a faster, more energy-efficient manufacturing process for high-performance thermoset composites. This numerical study focuses on the FP-based manufacturing of short-fiber-reinforced polymeric matrix composites. The investigation involves a combination of multiphysics finite element analyses and analytical predictions. The developed model is also applied to a short-fiber composite with spatially varying fiber orientation obtained from a sample produced by vacuum injection method. The results show how the steady-state front velocity and inclination angle depend on the fiber orientation angle and volume fraction. Analytical expressions are derived to capture that dependence and show excellent agreement with the numerical steady-state results. Simulations of FP in short-fiber composites based on experimental distributions of the fiber orientation indicate the feasibility of FP in samples prepared by injection molding.

quote

GB/T 7714-2015 [1] Tolga Topkaya, Yuan Gao, Philippe H. Geubelle. ACS Applied Polymer Materials, 2022(4). DOI:10.1021/acsapm.2c00818.
MLA [1] Tolga Topkaya, et al., ACS Applied Polymer Materials, no. 4, 2022, https://doi.org/10.1021/acsapm.2c00818.
APA [1] Tolga Topkaya, Yuan Gao, & Philippe H. Geubelle. (2022). ACS Applied Polymer Materials(4). https://doi.org/10.1021/acsapm.2c00818
IEEE [1] Tolga Topkaya, Yuan Gao, and Philippe H. Geubelle, ACS Applied Polymer Materials, no. 4, 2022, doi: 10.1021/acsapm.2c00818. keywords: {frontal polymerization;shortfiberreinforced composite;carbon fiber;finite element analysis;dicyclopentadiene}