daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Ultramicroporous Lonsdaleite Topology MOF with High Propane Uptake and Propane/Methane Selectivity for Propane Capture from Simulated Natural Gas AITranslate

University of Limerick; China University of Petroleum-Beijing; University of Limerick; University of Limerick; University of Limerick; University of Limerick; University of Limerick; China University of Petroleum-Beijing; University of Limerick; University of Limerick
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Propane (C3H8) is a widely used fuel gas. Metal–organic framework (MOF) physisorbents that are C3H8 selective offer the potential to significantly reduce the energy footprint for capturing C3H8 from natural gas, where C3H8 is typically present as a minor component. Here we report the C3H8 recovery performance of a previously unreported lonsdaleite, lon, topology MOF, a chiral metal–organic material, [Ni(S-IEDC)(bipy)(SCN)]n, CMOM-7. CMOM-7 was prepared from three low-cost precursors: Ni(SCN)2, S-indoline-2-carboxylic acid (S-IDECH), and 4,4′-bipyridine (bipy), and its structure was determined by single crystal X-ray crystallography. Pure gas adsorption isotherms revealed that CMOM-7 exhibited high C3H8 uptake (2.71 mmol g–1) at 0.05 bar, an indication of a higher affinity for C3H8 than both C2H6 and CH4. Dynamic column breakthrough experiments afforded high purity C3H8 capture from a gas mixture comprising C3H8/C2H6/CH4 (v/v/v = 5/10/85). Despite the dilute C3H8 stream, CMOM-7 registered a high dynamic uptake of C3H8 and a breakthrough time difference between C3H8 and C2H6 of 79.5 min g–1, superior to those of previous MOF physisorbents studied under the same flow rate. Analysis of crystallographic data and Grand Canonical Monte Carlo simulations provides insight into the two C3H8 binding sites in CMOM-7, both of which are driven by C–H···π and hydrogen bonding interactions.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsmaterialslett.3c01157

Chinese Library Classification Number:

Citation Information:

Propane (C3H8) is a widely used fuel gas. Metal–organic framework (MOF) physisorbents that are C3H8 selective offer the potential to significantly reduce the energy footprint for capturing C3H8 from natural gas, where C3H8 is typically present as a minor component. Here we report the C3H8 recovery performance of a previously unreported lonsdaleite, lon, topology MOF, a chiral metal–organic material, [Ni(S-IEDC)(bipy)(SCN)]n, CMOM-7. CMOM-7 was prepared from three low-cost precursors: Ni(SCN)2, S-indoline-2-carboxylic acid (S-IDECH), and 4,4′-bipyridine (bipy), and its structure was determined by single crystal X-ray crystallography. Pure gas adsorption isotherms revealed that CMOM-7 exhibited high C3H8 uptake (2.71 mmol g–1) at 0.05 bar, an indication of a higher affinity for C3H8 than both C2H6 and CH4. Dynamic column breakthrough experiments afforded high purity C3H8 capture from a gas mixture comprising C3H8/C2H6/CH4 (v/v/v = 5/10/85). Despite the dilute C3H8 stream, CMOM-7 registered a high dynamic uptake of C3H8 and a breakthrough time difference between C3H8 and C2H6 of 79.5 min g–1, superior to those of previous MOF physisorbents studied under the same flow rate. Analysis of crystallographic data and Grand Canonical Monte Carlo simulations provides insight into the two C3H8 binding sites in CMOM-7, both of which are driven by C–H···π and hydrogen bonding interactions.

quote

GB/T 7714-2015 [1] Chenghua Deng, Li Zhao, MeiYan Gao, et al. ACS Materials Letters, 2024(6). DOI:10.1021/acsmaterialslett.3c01157.
MLA [1] Chenghua Deng, et al., ACS Materials Letters, no. 6, 2024, https://doi.org/10.1021/acsmaterialslett.3c01157.
APA [1] Chenghua Deng, Li Zhao, MeiYan Gao, Shaza Darwish, BaiQiao Song, Debobroto Sensharma, Matteo Lusi, YunLei Peng, Soumya Mukherjee, & Michael J. Zaworotko. (2024). ACS Materials Letters(6). https://doi.org/10.1021/acsmaterialslett.3c01157
IEEE [1] Chenghua Deng, Li Zhao, MeiYan Gao, Shaza Darwish, BaiQiao Song, Debobroto Sensharma, Matteo Lusi, YunLei Peng, Soumya Mukherjee, and Michael J. Zaworotko, ACS Materials Letters, no. 6, 2024, doi: 10.1021/acsmaterialslett.3c01157.