Networking of Block Copolymer Nanoassemblies via Digital Light Processing Four-Dimensional Printing for Programmable Actuation AITranslate

Nanyang Technological University; Nanyang Technological University; Nanyang Technological University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Controls over stimuli-responsive functional materials and programmable shape deformations are key features in the four-dimensional (4D) printing of soft actuators. Instead of using random copolymers, homopolymers, or natural polymers, this paper reports the first use of amphiphilic, photocurable, and pH-responsive block copolymer (BCP) nanoassemblies in digital light processing (DLP) 4D printing to fabricate smart and programmable soft actuators. Programmable actuation was studied via a bottom-up approach: (1) designed synthesis of pH-responsive BCPs, (2) nanoassembly structures of BCPs, and (3) networking of nanoassemblies via the photocuring process in DLP. As a proof-of-concept, bilayered grippers, ring-shaped actuators, and octopus-like actuators were programmed to produce a range of bending angles and actuation patterns. pH-responsive BCP nanoassemblies were also combined with commercially available three-dimensional printing liquid resin (PlasClear) to produce stimulus-responsive printing ink that was successfully used for 4D printing applications. Thus, smart and programmable materials were developed for 4D printing applications.

KeyWords AITranslate

stimuliresponsive reversible shape change 3D printing block copolymer selfassembly
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.2c01617

Chinese Library Classification Number:

Citation Information:

Controls over stimuli-responsive functional materials and programmable shape deformations are key features in the four-dimensional (4D) printing of soft actuators. Instead of using random copolymers, homopolymers, or natural polymers, this paper reports the first use of amphiphilic, photocurable, and pH-responsive block copolymer (BCP) nanoassemblies in digital light processing (DLP) 4D printing to fabricate smart and programmable soft actuators. Programmable actuation was studied via a bottom-up approach: (1) designed synthesis of pH-responsive BCPs, (2) nanoassembly structures of BCPs, and (3) networking of nanoassemblies via the photocuring process in DLP. As a proof-of-concept, bilayered grippers, ring-shaped actuators, and octopus-like actuators were programmed to produce a range of bending angles and actuation patterns. pH-responsive BCP nanoassemblies were also combined with commercially available three-dimensional printing liquid resin (PlasClear) to produce stimulus-responsive printing ink that was successfully used for 4D printing applications. Thus, smart and programmable materials were developed for 4D printing applications.

quote

GB/T 7714-2015 [1] Houwen Matthew Pan, Jit Sarkar, Atsushi Goto. ACS Applied Polymer Materials, 2022(4). DOI:10.1021/acsapm.2c01617.
MLA [1] Houwen Matthew Pan, et al., ACS Applied Polymer Materials, no. 4, 2022, https://doi.org/10.1021/acsapm.2c01617.
APA [1] Houwen Matthew Pan, Jit Sarkar, & Atsushi Goto. (2022). ACS Applied Polymer Materials(4). https://doi.org/10.1021/acsapm.2c01617
IEEE [1] Houwen Matthew Pan, Jit Sarkar, and Atsushi Goto, ACS Applied Polymer Materials, no. 4, 2022, doi: 10.1021/acsapm.2c01617. keywords: {stimuliresponsive;reversible shape change;3D printing;block copolymer;selfassembly}