daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Coassembling Hydroxypropyl Cellulose into a Chiral Nematic Composite and Patternization with a Photomask and Direct Ink Writing AITranslate

Nanjing Forestry University; Nanjing Forestry University; Nanjing Forestry University;Qilu University of Technology; Nanjing Forestry University; South China Normal University; University of New Brunswick; Nanjing Forestry University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Additive manufacturing (AM) is a next-generation technique for engineering hierarchically structured materials. The development of sustainable ink materials for AM is imperative. In this work, we explored hydroxypropyl cellulose (HPC) as a sustainable photonic ink for patterning by photomask and direct ink writing techniques. Specifically, we comprehensively investigated the coassembly behavior of HPC with a guest monomer into a chiral nematic structure and the parameters that affect the transition from a solution to composite film of HPC/monomer. The results reveal that the HPC/monomer has the ability to form a chiral nematic structure, and such a hierarchical structure can reflect light with a specific wavelength. The helical pitch in the chiral nematic structure, corresponding to the reflected wavelength, can be modulated via HPC concentration, the addition amount of monomer, cross-linking time, and drying temperature. Additionally, the composite exhibits robust mechanical properties and is capable of tolerating a wet environment (both high relative humidity and water). This comprehensive study is a fascinating example of using a sustainable cellulose derivative as a 3D printing ink and provides powerful support for the development of structural color materials.

KeyWords AITranslate

photonic ink sustainability hydroxypropyl cellulose (HPC) chiral nematic structure additive manufacturing
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.3c02115

Chinese Library Classification Number:

Citation Information:

Additive manufacturing (AM) is a next-generation technique for engineering hierarchically structured materials. The development of sustainable ink materials for AM is imperative. In this work, we explored hydroxypropyl cellulose (HPC) as a sustainable photonic ink for patterning by photomask and direct ink writing techniques. Specifically, we comprehensively investigated the coassembly behavior of HPC with a guest monomer into a chiral nematic structure and the parameters that affect the transition from a solution to composite film of HPC/monomer. The results reveal that the HPC/monomer has the ability to form a chiral nematic structure, and such a hierarchical structure can reflect light with a specific wavelength. The helical pitch in the chiral nematic structure, corresponding to the reflected wavelength, can be modulated via HPC concentration, the addition amount of monomer, cross-linking time, and drying temperature. Additionally, the composite exhibits robust mechanical properties and is capable of tolerating a wet environment (both high relative humidity and water). This comprehensive study is a fascinating example of using a sustainable cellulose derivative as a 3D printing ink and provides powerful support for the development of structural color materials.

quote

GB/T 7714-2015 [1] Shihao Wang, Yungeng Qi, Shasha Wang, et al. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.3c02115.
MLA [1] Shihao Wang, et al., ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.3c02115.
APA [1] Shihao Wang, Yungeng Qi, Shasha Wang, Guihua Yang, Junlong Song, Zhen Zhang, Huining Xiao, & Jiaqi Guo. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.3c02115
IEEE [1] Shihao Wang, Yungeng Qi, Shasha Wang, Guihua Yang, Junlong Song, Zhen Zhang, Huining Xiao, and Jiaqi Guo, ACS Applied Polymer Materials, no. 5, 2023, doi: 10.1021/acsapm.3c02115. keywords: {photonic ink;sustainability;hydroxypropyl cellulose (HPC);chiral nematic structure;additive manufacturing}