Heteroatom-Doped Transition Metal Electrocatalysts for Hydrogen Evolution Reaction AITranslate
Abstract AITranslate
Developing efficient and low-cost electrocatalysts for the hydrogen evolution reaction (HER) is important for clean energy systems. Non-noble transition metals are the most promising candidates for replacement of conventional Pt group catalysts for the HER. However, most non-noble metals show poor HER activity due to their intrinsic electronic structures. Herein, we use a multifaceted heteroatom doping method (nitrogen, sulfur, and phosphorus) to directly and continuously fine-tune the electronic structure and HER activity of non-noble metals without changing their chemical composition. As a proof-of-concept, a nitrogen and phosphorus dual-doped Ni catalyst is explored by precisely manipulating doping modes, revealing the best HER performance among all doped Ni catalysts tested. The doping-induced charge redistribution in the Ni metal significantly influences its catalytic performance for the HER in alkaline media, which is confirmed by merging theoretical calculation with synchrotron-based spectroscopy. The principle that can bridge the doping modes and HER activity of the doped catalysts is built with a volcano relationship.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsenergylett.9b00348
Chinese Library Classification Number:
Citation Information:
Developing efficient and low-cost electrocatalysts for the hydrogen evolution reaction (HER) is important for clean energy systems. Non-noble transition metals are the most promising candidates for replacement of conventional Pt group catalysts for the HER. However, most non-noble metals show poor HER activity due to their intrinsic electronic structures. Herein, we use a multifaceted heteroatom doping method (nitrogen, sulfur, and phosphorus) to directly and continuously fine-tune the electronic structure and HER activity of non-noble metals without changing their chemical composition. As a proof-of-concept, a nitrogen and phosphorus dual-doped Ni catalyst is explored by precisely manipulating doping modes, revealing the best HER performance among all doped Ni catalysts tested. The doping-induced charge redistribution in the Ni metal significantly influences its catalytic performance for the HER in alkaline media, which is confirmed by merging theoretical calculation with synchrotron-based spectroscopy. The principle that can bridge the doping modes and HER activity of the doped catalysts is built with a volcano relationship.
quote
| GB/T 7714-2015 | [1] Huanyu Jin, Xin Liu, Shuangming Chen, et al. ACS Energy Letters, 2019(4). DOI:10.1021/acsenergylett.9b00348. |
| MLA | [1] Huanyu Jin, et al., ACS Energy Letters, no. 4, 2019, https://doi.org/10.1021/acsenergylett.9b00348. |
| APA | [1] Huanyu Jin, Xin Liu, Shuangming Chen, Anthony Vasileff, Laiquan Li, Yan Jiao, Li Song, Yao Zheng, & ShiZhang Qiao. (2019). ACS Energy Letters(4). https://doi.org/10.1021/acsenergylett.9b00348 |
| IEEE | [1] Huanyu Jin, Xin Liu, Shuangming Chen, Anthony Vasileff, Laiquan Li, Yan Jiao, Li Song, Yao Zheng, and ShiZhang Qiao, ACS Energy Letters, no. 4, 2019, doi: 10.1021/acsenergylett.9b00348. |