Lightweight Aramid Nanofiber Aerogel with a Hierarchical Cellular Structure for Thermal Insulation AITranslate

Tiangong University; Tiangong University; Tiangong University; Tiangong University;Yantai Metastar Special Paper Co., Ltd.; Tiangong University; Tiangong University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Excellent insulation materials are urgently needed to insulate or reduce thermal transfer. However, the creation of such materials with ultralow thermal conductivity, high temperature tolerance, and mechanical robustness still faces enormous challenges. Here, a lightweight and robust aramid nanofiber (ANF) aerogel with a hierarchical cellular framework is reported by physically isolate ANFs from poly(p-phenylene terephthalamide) fibers, directional freezing of ANFs to cellular structure, and establishing chemical bonding of ANFs. Given the synergistic effect, the resulting aerogel exhibits a low thermal conductivity of 23.7 mW m–1 K–1, a low density of 1.42 mg cm–3, a high porosity of 90%, and a high compressive strain of up to 90%, indicating its excellent overall performance. The successful synthesis of the ANF aerogel may provide insights into the development of lightweight, flexible, and structurally adaptable thermal insulators.

KeyWords AITranslate

aerogel aramid nanofiber highpressure homogenization directional freezing hierarchical cellular structure thermal insulation
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.2c01566

Chinese Library Classification Number:

Citation Information:

Excellent insulation materials are urgently needed to insulate or reduce thermal transfer. However, the creation of such materials with ultralow thermal conductivity, high temperature tolerance, and mechanical robustness still faces enormous challenges. Here, a lightweight and robust aramid nanofiber (ANF) aerogel with a hierarchical cellular framework is reported by physically isolate ANFs from poly(p-phenylene terephthalamide) fibers, directional freezing of ANFs to cellular structure, and establishing chemical bonding of ANFs. Given the synergistic effect, the resulting aerogel exhibits a low thermal conductivity of 23.7 mW m–1 K–1, a low density of 1.42 mg cm–3, a high porosity of 90%, and a high compressive strain of up to 90%, indicating its excellent overall performance. The successful synthesis of the ANF aerogel may provide insights into the development of lightweight, flexible, and structurally adaptable thermal insulators.

quote

GB/T 7714-2015 [1] Lei Shi, Yuan Lin, Shan Huan, et al. ACS Applied Polymer Materials, 2022(4). DOI:10.1021/acsapm.2c01566.
MLA [1] Lei Shi, et al., ACS Applied Polymer Materials, no. 4, 2022, https://doi.org/10.1021/acsapm.2c01566.
APA [1] Lei Shi, Yuan Lin, Shan Huan, Guodong Zhao, Ming Jiang, Ya Liu, & Xupin Zhuang. (2022). ACS Applied Polymer Materials(4). https://doi.org/10.1021/acsapm.2c01566
IEEE [1] Lei Shi, Yuan Lin, Shan Huan, Guodong Zhao, Ming Jiang, Ya Liu, and Xupin Zhuang, ACS Applied Polymer Materials, no. 4, 2022, doi: 10.1021/acsapm.2c01566. keywords: {aerogel;aramid nanofiber;highpressure homogenization;directional freezing;hierarchical cellular structure;thermal insulation}