Effect of Poly(vinylphenol) on the Ferroelectric Performance of Poly(vinylidene fluoride-trifluoroethylene) AITranslate

Beijing University of Chemical Technology; Beijing University of Chemical Technology; Beijing University of Chemical Technology; Beijing University of Chemical Technology; Beijing University of Chemical Technology; Qingdao University of Science & Technology
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Structures and ferroelectric properties of poly(vinylidene fluoride-trifluoroethylene)/poly(vinylphenol), i.e., P(VDF-TrFE)/PVPh, blends are studied. It is found that a small amount of PVPh segregates as small nanodomains distributed homogeneously on the surface of a P(VDF-TrFE) film. The incorporation of PVPh depresses the Curie transition temperature and remnant polarization of P(VDF-TrFE) slightly. It enhances the coercive electric field (Ec) slightly but improves the thermal stability of ferroelectric properties by nearly 30 °C with 5 wt % PVPh. In addition, by maintaining the relatively high permittivity, the addition of PVPh effectively lowers the dielectric losses. This provides an efficient and simple way to fabricate P(VDF-TrFE)-based nonvolatile flexible memories with low leakage, high thermal stability, and high breakdown strength.

KeyWords AITranslate

poly(vinylidene fluoridetrifluoroethylene) poly(vinylphenol) blend ferroelectric nonvolatile
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.9b00060

Chinese Library Classification Number:

Citation Information:

Structures and ferroelectric properties of poly(vinylidene fluoride-trifluoroethylene)/poly(vinylphenol), i.e., P(VDF-TrFE)/PVPh, blends are studied. It is found that a small amount of PVPh segregates as small nanodomains distributed homogeneously on the surface of a P(VDF-TrFE) film. The incorporation of PVPh depresses the Curie transition temperature and remnant polarization of P(VDF-TrFE) slightly. It enhances the coercive electric field (Ec) slightly but improves the thermal stability of ferroelectric properties by nearly 30 °C with 5 wt % PVPh. In addition, by maintaining the relatively high permittivity, the addition of PVPh effectively lowers the dielectric losses. This provides an efficient and simple way to fabricate P(VDF-TrFE)-based nonvolatile flexible memories with low leakage, high thermal stability, and high breakdown strength.

quote

GB/T 7714-2015 [1] Ce Mi, Nan Gao, Huihui Li, et al. ACS Applied Polymer Materials, 2019(1). DOI:10.1021/acsapm.9b00060.
MLA [1] Ce Mi, et al., ACS Applied Polymer Materials, no. 1, 2019, https://doi.org/10.1021/acsapm.9b00060.
APA [1] Ce Mi, Nan Gao, Huihui Li, Junteng Liu, Xiaoli Sun, & Shouke Yan. (2019). ACS Applied Polymer Materials(1). https://doi.org/10.1021/acsapm.9b00060
IEEE [1] Ce Mi, Nan Gao, Huihui Li, Junteng Liu, Xiaoli Sun, and Shouke Yan, ACS Applied Polymer Materials, no. 1, 2019, doi: 10.1021/acsapm.9b00060. keywords: {poly(vinylidene fluoridetrifluoroethylene);poly(vinylphenol);blend;ferroelectric;nonvolatile}