daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Synthesis and Deformable Hierarchical Nanostructure of Intrinsically Stretchable ABA Triblock Copolymer Composed of Poly(3-hexylthiophene) and Polyisobutylene Segments AITranslate

Yamagata University; Yamagata University; Yamagata University; Yamagata University;Chemicals R&D Group, HPM Research & Development Department;Japan Synchrotron Radiation Research Institute; Hiroshima University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

A novel intrinsically stretchable ABA triblock copolymer can be synthesized where A and B are poly(3-hexylthiophene) (P3HT) and polyisobutylene (PIB) segments, respectively. The deformation of the self-assembled hierarchical nanostructure of the block copolymer thin film was clearly observed by grazing incidence small- and wide-angle X-ray scattering.

KeyWords AITranslate

Nanostructure block copolymer poly(3hexylthiophene) polyisobutylene stretchable selfassembly
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.8b00087

Chinese Library Classification Number:

Citation Information:

A novel intrinsically stretchable ABA triblock copolymer can be synthesized where A and B are poly(3-hexylthiophene) (P3HT) and polyisobutylene (PIB) segments, respectively. The deformation of the self-assembled hierarchical nanostructure of the block copolymer thin film was clearly observed by grazing incidence small- and wide-angle X-ray scattering.

quote

GB/T 7714-2015 [1] Tomoya Higashihara, Seijiro Fukuta, Yuto Ochiai, et al. ACS Applied Polymer Materials, 2019(1). DOI:10.1021/acsapm.8b00087.
MLA [1] Tomoya Higashihara, et al., ACS Applied Polymer Materials, no. 1, 2019, https://doi.org/10.1021/acsapm.8b00087.
APA [1] Tomoya Higashihara, Seijiro Fukuta, Yuto Ochiai, Tomohito Sekine, Keisuke Chino, Tomoyuki Koganezawa, & Itaru Osaka. (2019). ACS Applied Polymer Materials(1). https://doi.org/10.1021/acsapm.8b00087
IEEE [1] Tomoya Higashihara, Seijiro Fukuta, Yuto Ochiai, Tomohito Sekine, Keisuke Chino, Tomoyuki Koganezawa, and Itaru Osaka, ACS Applied Polymer Materials, no. 1, 2019, doi: 10.1021/acsapm.8b00087. keywords: {Nanostructure;block copolymer;poly(3hexylthiophene);polyisobutylene;stretchable;selfassembly}