InSb: A Stable Cycling Anode Material Enables Fast Charging of Li-Ion Batteries at Sub-zero Temperatures AITranslate
Abstract AITranslate
In this work we surprisingly find that the reaction mechanism, Li-ion diffusion kinetics, and polycrystalline sphalerite structure of the InSb anode materials remain unchanged during the charging and discharging process at both room and sub-zero temperatures. The sputtered pure InSb film anodes can stably cycle more than 800 times at 1 A/g and deliver a high capacity of 534.6 mAh/g at 30 °C. With a high current rate of 2 A/g at −40 °C, a capacity of 402.8 mAh/g can be maintained. For the ball-milled InSb/graphite composite, a capacity of 434.3 mAh/g at 1 A/g can remain very stable for more than 700 cycles at both 30 °C and −50 °C. The 2500 mAh soft pack cells, which are made entirely from the commercialization process and successfully run long-term at −30 °C, also demonstrate the potential of InSb anodes for commercial applications.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsenergylett.3c00690
Chinese Library Classification Number:
Citation Information:
In this work we surprisingly find that the reaction mechanism, Li-ion diffusion kinetics, and polycrystalline sphalerite structure of the InSb anode materials remain unchanged during the charging and discharging process at both room and sub-zero temperatures. The sputtered pure InSb film anodes can stably cycle more than 800 times at 1 A/g and deliver a high capacity of 534.6 mAh/g at 30 °C. With a high current rate of 2 A/g at −40 °C, a capacity of 402.8 mAh/g can be maintained. For the ball-milled InSb/graphite composite, a capacity of 434.3 mAh/g at 1 A/g can remain very stable for more than 700 cycles at both 30 °C and −50 °C. The 2500 mAh soft pack cells, which are made entirely from the commercialization process and successfully run long-term at −30 °C, also demonstrate the potential of InSb anodes for commercial applications.
quote
| GB/T 7714-2015 | [1] Xingyu Xiong, Gang Zhou, Hechuan Yu, et al. ACS Energy Letters, 2023(8). DOI:10.1021/acsenergylett.3c00690. |
| MLA | [1] Xingyu Xiong, et al., ACS Energy Letters, no. 8, 2023, https://doi.org/10.1021/acsenergylett.3c00690. |
| APA | [1] Xingyu Xiong, Gang Zhou, Hechuan Yu, Xuexia Lan, Fanbo Meng, & Renzong Hu. (2023). ACS Energy Letters(8). https://doi.org/10.1021/acsenergylett.3c00690 |
| IEEE | [1] Xingyu Xiong, Gang Zhou, Hechuan Yu, Xuexia Lan, Fanbo Meng, and Renzong Hu, ACS Energy Letters, no. 8, 2023, doi: 10.1021/acsenergylett.3c00690. |