Ir–O–V Catalytic Group in Ir-Doped NiV(OH)2 for Overall Water Splitting AITranslate

Tianjin University; Tianjin University; Tianjin University; Tianjin University; Tianjin University; Tianjin University; Tianjin University; Tianjin University; Tianjin University; Japan|Far Eastern Federal University; Tianjin University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Bifunctional electrocatalysts for both hydrogen evolution reaction (HER) and oxygen evolution reaction (OER) are very crucial for converting water into clean fuel through overall water splitting. Here, we report on a bifunctional catalyst based on Ir-doped NiV layered double hydroxide with Ir–O–V catalytic groups on which water dissociation, HER, and OER occur on Ir, bridge O, and V atoms, respectively. Interestingly, the dopant Ir ions were found to play a triple role: (i) serve as catalytic sites for water dissociation, (ii) reduce charge density on adjacent bridge oxygen, thus facilitating HER there, and (iii) increase charge density on V ions, which in turn boosts OER. As a result, the catalyst achieves an ultralow applied voltage for overall water splitting (1.49 V @ 10 mA cm–2) and beats the noble metallic couple Pt/C and Ir/C with its value of 1.60 V @ 10 mA cm–2.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.9b01252

Chinese Library Classification Number:

Citation Information:

Bifunctional electrocatalysts for both hydrogen evolution reaction (HER) and oxygen evolution reaction (OER) are very crucial for converting water into clean fuel through overall water splitting. Here, we report on a bifunctional catalyst based on Ir-doped NiV layered double hydroxide with Ir–O–V catalytic groups on which water dissociation, HER, and OER occur on Ir, bridge O, and V atoms, respectively. Interestingly, the dopant Ir ions were found to play a triple role: (i) serve as catalytic sites for water dissociation, (ii) reduce charge density on adjacent bridge oxygen, thus facilitating HER there, and (iii) increase charge density on V ions, which in turn boosts OER. As a result, the catalyst achieves an ultralow applied voltage for overall water splitting (1.49 V @ 10 mA cm–2) and beats the noble metallic couple Pt/C and Ir/C with its value of 1.60 V @ 10 mA cm–2.

quote

GB/T 7714-2015 [1] Shuang Li, Cong Xi, YongZhen Jin, et al. ACS Energy Letters, 2019(4). DOI:10.1021/acsenergylett.9b01252.
MLA [1] Shuang Li, et al., ACS Energy Letters, no. 4, 2019, https://doi.org/10.1021/acsenergylett.9b01252.
APA [1] Shuang Li, Cong Xi, YongZhen Jin, Deyao Wu, JiaQi Wang, Tao Liu, HaiBin Wang, CunKu Dong, Hui Liu, Sergei A. Kulinich, & XiWen Du. (2019). ACS Energy Letters(4). https://doi.org/10.1021/acsenergylett.9b01252