Nanoparticle Diffusion and Fixation for the Preparation of Durable Transparent Superhydrophobic Coatings AITranslate
Abstract AITranslate
Due to the size limitation of nanostructures in transparent superhydrophobic (TS) coatings, it is a formidable challenge to construct a TS coating with acceptable mechanical durability. The matrix should connect with nanoparticles and the substrate with more chemical bonds to provide the essential mechanical robustness of the coating layer. In this study, methylacryloxypropyltrimethoxysilane (MEMO) that has three Si–OCH3 groups was polymerized to PMEMO and used as an “ideal” adhesive for the fabrication of durable transparent superhydrophobic (DTS) coatings. Hydrophobic SiO2 nanoparticles were fixed through diffusion into the swollen PMEMO network to avoid the micro-roughness caused by agglomeration. The light transmission of the glass slide after coating with PMEMO/SiO2 was 89.24%. The coating layer maintained its superhydrophobicity with the impact resistance of 160 g of sand and 4.6 m/s water jet for 360 s and heat treatment under 200 °C. The green, non-toxic, and non-fluorinated coating preparation method is universal and scalable, which has promising and large-scale application prospects.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsapm.3c00671
Chinese Library Classification Number:
Citation Information:
Due to the size limitation of nanostructures in transparent superhydrophobic (TS) coatings, it is a formidable challenge to construct a TS coating with acceptable mechanical durability. The matrix should connect with nanoparticles and the substrate with more chemical bonds to provide the essential mechanical robustness of the coating layer. In this study, methylacryloxypropyltrimethoxysilane (MEMO) that has three Si–OCH3 groups was polymerized to PMEMO and used as an “ideal” adhesive for the fabrication of durable transparent superhydrophobic (DTS) coatings. Hydrophobic SiO2 nanoparticles were fixed through diffusion into the swollen PMEMO network to avoid the micro-roughness caused by agglomeration. The light transmission of the glass slide after coating with PMEMO/SiO2 was 89.24%. The coating layer maintained its superhydrophobicity with the impact resistance of 160 g of sand and 4.6 m/s water jet for 360 s and heat treatment under 200 °C. The green, non-toxic, and non-fluorinated coating preparation method is universal and scalable, which has promising and large-scale application prospects.
quote
| GB/T 7714-2015 | [1] Runyu Wang, Chuanshuang Hu, Jiewen Li, et al. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.3c00671. |
| MLA | [1] Runyu Wang, et al., ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.3c00671. |
| APA | [1] Runyu Wang, Chuanshuang Hu, Jiewen Li, Xiuyi Lin, & Weiwei Zhang. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.3c00671 |
| IEEE | [1] Runyu Wang, Chuanshuang Hu, Jiewen Li, Xiuyi Lin, and Weiwei Zhang, ACS Applied Polymer Materials, no. 5, 2023, doi: 10.1021/acsapm.3c00671. keywords: {durable;transparent;superhydrophobic;nanoSiO2;coating} |