daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Tough and Biocompatible Hydrogel Tissue Adhesives Entirely Based on Naturally Derived Ingredients AITranslate

Southern University of Science and Technology; Tsinghua University; Southern University of Science and Technology; Southern University of Science and Technology; Tsinghua University;Suzhou Soft Intelligent Materials Co. Ltd.; Yale University; Southern University of Science and Technology
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Hydrogel tissue adhesives have tremendous potential applications in biological engineering. Existing hydrogel tissue adhesives generally do not have adequate mechanical robustness and acceptable biocompatibility at the same time. Herein, we report a one-step method to synthesize tough and biocompatible hydrogel tissue adhesives entirely made of naturally derived ingredients. We select two natural polymers, chitosan and gelatin, to construct the backbone and a bioderived compound, genipin, as the cross-linker. We show that, upon gelation, genipins cross-link chitosan and gelatin to form two interpenetrated networks and interlink them to tissue surfaces. Meanwhile, hydrogen bonds form in the matrix to strengthen the networks and at the interface to strengthen the adhesion between the hydrogel and tissue. Furthermore, we elaborately use high initial polymer contents to induce topological entanglements in the polymer networks to toughen the hydrogel. The resulting chitosan–gelatin hydrogel provides a tough matrix, and the robust covalent interlinks and hydrogen bonds provide a strong interface, achieving a tensile strength of ∼190 kPa, a fracture toughness of 205.7 J/m2, a mode I adhesion energy of 197.6 J/m2, and a mode II adhesion energy of 51.2 J/m2. We demonstrate that the hydrogel tissue adhesive is injectable, degradable, and noncytotoxic and can be used for the controlled release of the anticancer drug cisplatin. All-natural ingredient-based tough and biocompatible hydrogels are promising as tissue adhesives for biomedical and related applications.

KeyWords AITranslate

hydrogel tissue adhesive natural polymer toughness biocompatibility
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.3c01926

Chinese Library Classification Number:

Citation Information:

Hydrogel tissue adhesives have tremendous potential applications in biological engineering. Existing hydrogel tissue adhesives generally do not have adequate mechanical robustness and acceptable biocompatibility at the same time. Herein, we report a one-step method to synthesize tough and biocompatible hydrogel tissue adhesives entirely made of naturally derived ingredients. We select two natural polymers, chitosan and gelatin, to construct the backbone and a bioderived compound, genipin, as the cross-linker. We show that, upon gelation, genipins cross-link chitosan and gelatin to form two interpenetrated networks and interlink them to tissue surfaces. Meanwhile, hydrogen bonds form in the matrix to strengthen the networks and at the interface to strengthen the adhesion between the hydrogel and tissue. Furthermore, we elaborately use high initial polymer contents to induce topological entanglements in the polymer networks to toughen the hydrogel. The resulting chitosan–gelatin hydrogel provides a tough matrix, and the robust covalent interlinks and hydrogen bonds provide a strong interface, achieving a tensile strength of ∼190 kPa, a fracture toughness of 205.7 J/m2, a mode I adhesion energy of 197.6 J/m2, and a mode II adhesion energy of 51.2 J/m2. We demonstrate that the hydrogel tissue adhesive is injectable, degradable, and noncytotoxic and can be used for the controlled release of the anticancer drug cisplatin. All-natural ingredient-based tough and biocompatible hydrogels are promising as tissue adhesives for biomedical and related applications.

quote

GB/T 7714-2015 [1] Ziyi Xu, Haihui Zhang, Yuan Huang, et al. ACS Applied Polymer Materials, 2024(6). DOI:10.1021/acsapm.3c01926.
MLA [1] Ziyi Xu, et al., ACS Applied Polymer Materials, no. 6, 2024, https://doi.org/10.1021/acsapm.3c01926.
APA [1] Ziyi Xu, Haihui Zhang, Yuan Huang, Hao Zhong, Peiwu Qin, Sibo Cheng, Yuenan Wang, & Canhui Yang. (2024). ACS Applied Polymer Materials(6). https://doi.org/10.1021/acsapm.3c01926
IEEE [1] Ziyi Xu, Haihui Zhang, Yuan Huang, Hao Zhong, Peiwu Qin, Sibo Cheng, Yuenan Wang, and Canhui Yang, ACS Applied Polymer Materials, no. 6, 2024, doi: 10.1021/acsapm.3c01926. keywords: {hydrogel;tissue adhesive;natural polymer;toughness;biocompatibility}