Stimuli responsiveness, propulsion and application of the stimuli-responsive polymer based micromotor AITranslate
Abstract AITranslate
In the past decade, the field of micromotor has undergone tremendous progresses. The autonomous and controlled motion of the micromotors inside a liquid environment makes them potentially attractive for various fields including environmental remediation, the biomedical application, etc. In addition to the micromotors based on non-responsive materials, those based on stimuli-responsive polymers have recently attracted more and more attentions due to their functional versatility and stimuli responsiveness. In this review, we summarize the recent advances in the field of stimuli-responsive polymer based micromotor. Based on the stimuli responsiveness originating from the stimuli-responsive polymer components inside the micromotors, we highlight the unprecedented properties of the stimuli-responsive polymer based micromotors and elaborate the potential applications in various fields ranging from sensing to logic gate and the biomedical field, etc.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1016/j.apmt.2021.101250
Chinese Library Classification Number:
Citation Information:
In the past decade, the field of micromotor has undergone tremendous progresses. The autonomous and controlled motion of the micromotors inside a liquid environment makes them potentially attractive for various fields including environmental remediation, the biomedical application, etc. In addition to the micromotors based on non-responsive materials, those based on stimuli-responsive polymers have recently attracted more and more attentions due to their functional versatility and stimuli responsiveness. In this review, we summarize the recent advances in the field of stimuli-responsive polymer based micromotor. Based on the stimuli responsiveness originating from the stimuli-responsive polymer components inside the micromotors, we highlight the unprecedented properties of the stimuli-responsive polymer based micromotors and elaborate the potential applications in various fields ranging from sensing to logic gate and the biomedical field, etc.
quote
| GB/T 7714-2015 | [1] Dalei Wang, Xiaoxia Han, Bin Dong, et al. Applied Materials Today, 2021(25). DOI:10.1016/j.apmt.2021.101250. |
| MLA | [1] Dalei Wang, et al., Applied Materials Today, no. 25, 2021, https://doi.org/10.1016/j.apmt.2021.101250. |
| APA | [1] Dalei Wang, Xiaoxia Han, Bin Dong, & Feng Shi. (2021). Applied Materials Today(25). https://doi.org/10.1016/j.apmt.2021.101250 |
| IEEE | [1] Dalei Wang, Xiaoxia Han, Bin Dong, and Feng Shi, Applied Materials Today, no. 25, 2021, doi: 10.1016/j.apmt.2021.101250. |