Aqueous Magnesium Zinc Hybrid Battery: An Advanced High-Voltage and High-Energy MgMn2O4 Cathode AITranslate
Abstract AITranslate
Driven by energy demand and commercial necessities, rechargeable aqueous metal ion batteries (RAMBs) have gained increasing attention over the last few decades as high-power and high-energy hubs for large-scale and ecofriendly energy storage devices (ESDs). However, recently explored RAMBs still do not provide the performance needed in order to be realized in grid-scale storage operations due to their poor electrochemical stability, low capacity, low working voltage, and apparently low specific energies. Herein, we have fabricated a new RAMB using MgMn2O4 as the cathode and zinc as the anode for the first time. The stable electrochemical performance of this RAMB at high current rates (∼80% capacity retention at 500 mA g–1 after 500 cycles) and a very high specific energy of 370 Wh kg–1 at a specific power of 70 W kg–1 make this newcomer to the family of RAMBs a serious contender for the exploration of safe and green ESDs in the near future.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsenergylett.8b01105
Chinese Library Classification Number:
Citation Information:
Driven by energy demand and commercial necessities, rechargeable aqueous metal ion batteries (RAMBs) have gained increasing attention over the last few decades as high-power and high-energy hubs for large-scale and ecofriendly energy storage devices (ESDs). However, recently explored RAMBs still do not provide the performance needed in order to be realized in grid-scale storage operations due to their poor electrochemical stability, low capacity, low working voltage, and apparently low specific energies. Herein, we have fabricated a new RAMB using MgMn2O4 as the cathode and zinc as the anode for the first time. The stable electrochemical performance of this RAMB at high current rates (∼80% capacity retention at 500 mA g–1 after 500 cycles) and a very high specific energy of 370 Wh kg–1 at a specific power of 70 W kg–1 make this newcomer to the family of RAMBs a serious contender for the exploration of safe and green ESDs in the near future.
quote
| GB/T 7714-2015 | [1] Vaiyapuri Soundharrajan, Balaji Sambandam, Sungjin Kim, et al. ACS Energy Letters, 2018(3). DOI:10.1021/acsenergylett.8b01105. |
| MLA | [1] Vaiyapuri Soundharrajan, et al., ACS Energy Letters, no. 3, 2018, https://doi.org/10.1021/acsenergylett.8b01105. |
| APA | [1] Vaiyapuri Soundharrajan, Balaji Sambandam, Sungjin Kim, Vinod Mathew, Jeonggeun Jo, Seokhun Kim, Jun Lee, Saiful Islam, Kwangho Kim, YangKook Sun, & Jaekook Kim. (2018). ACS Energy Letters(3). https://doi.org/10.1021/acsenergylett.8b01105 |
| IEEE | [1] Vaiyapuri Soundharrajan, Balaji Sambandam, Sungjin Kim, Vinod Mathew, Jeonggeun Jo, Seokhun Kim, Jun Lee, Saiful Islam, Kwangho Kim, YangKook Sun, and Jaekook Kim, ACS Energy Letters, no. 3, 2018, doi: 10.1021/acsenergylett.8b01105. |