Effective Chemical Prelithiation Strategy for Building a Silicon/Sulfur Li-Ion Battery AITranslate

Wuhan University; Wuhan University; Wuhan University; Wuhan University;Global Energy Interconnection Research Institute North America; Wuhan University; Wuhan University;National Engineering Research Center of Advanced Energy Storage Materials; Wuhan University; Wuhan University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Prelithiation has important applications to convert a nonlithiated cathode or anode materials into a controllably lithiated state required for developing advanced Li-ion batteries. However, most of the prelithiation reagents developed so far are highly reactive and sensitive to oxygen and moisture and therefore difficult for practical battery application. In this work, we developed a facile prelithiation strategy using lithium naphthalenide to fully prelithiate sulfur–poly(acrylonitrile) (S-PAN) composite into a Li2S-PAN cathode and to partially prelithiate nanosilicon into a LixSi anode, which leads to a new version of silicon/sulfur Li-ion battery. This LixSi/Li2S-PAN battery can demonstrate a high specific energy of 710 Wh kg–1, with a high initial Coulombic efficiency of 93.5% and a considerable cyclability. Also, this chemical prelithiation approach is mild, efficient, and widely applicable to a large range of Li-deficient electrodes, opening up new possibilities for development of low cost, environmentally benign, and high capacity Li-ion batteries.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.9b00889

Chinese Library Classification Number:

Citation Information:

Prelithiation has important applications to convert a nonlithiated cathode or anode materials into a controllably lithiated state required for developing advanced Li-ion batteries. However, most of the prelithiation reagents developed so far are highly reactive and sensitive to oxygen and moisture and therefore difficult for practical battery application. In this work, we developed a facile prelithiation strategy using lithium naphthalenide to fully prelithiate sulfur–poly(acrylonitrile) (S-PAN) composite into a Li2S-PAN cathode and to partially prelithiate nanosilicon into a LixSi anode, which leads to a new version of silicon/sulfur Li-ion battery. This LixSi/Li2S-PAN battery can demonstrate a high specific energy of 710 Wh kg–1, with a high initial Coulombic efficiency of 93.5% and a considerable cyclability. Also, this chemical prelithiation approach is mild, efficient, and widely applicable to a large range of Li-deficient electrodes, opening up new possibilities for development of low cost, environmentally benign, and high capacity Li-ion batteries.

quote

GB/T 7714-2015 [1] Yifei Shen, Jingmin Zhang, Yongfeng Pu, et al. ACS Energy Letters, 2019(4). DOI:10.1021/acsenergylett.9b00889.
MLA [1] Yifei Shen, et al., ACS Energy Letters, no. 4, 2019, https://doi.org/10.1021/acsenergylett.9b00889.
APA [1] Yifei Shen, Jingmin Zhang, Yongfeng Pu, Hui Wang, Bo Wang, Jiangfeng Qian, Yuliang Cao, Faping Zhong, Xinping Ai, & Hanxi Yang. (2019). ACS Energy Letters(4). https://doi.org/10.1021/acsenergylett.9b00889
IEEE [1] Yifei Shen, Jingmin Zhang, Yongfeng Pu, Hui Wang, Bo Wang, Jiangfeng Qian, Yuliang Cao, Faping Zhong, Xinping Ai, and Hanxi Yang, ACS Energy Letters, no. 4, 2019, doi: 10.1021/acsenergylett.9b00889.