Hierarchical Amine-Functionalized ZIF-8 Mixed-Matrix Membranes with an Engineered Interface and Transport Pathway for Efficient Gas Separation AITranslate
Abstract AITranslate
Herein, we report a facile approach to engineer a metal–organic framework (MOF) structure and polymer–MOF interface in a mixed-matrix membrane (MMM) to achieve high gas separation performance and plasticization resistance. Hierarchical ZIF-8-NH2 nanoparticles with a relatively small concentration of amine functionality (∼5 mol %) were prepared. The hierarchical MOF structure provides fast molecular transport pathways because of the MOF–MOF percolated network and high MOF packing density. Moreover, the interfacial interaction between the 6FDA-DAM:DABA(3:2) polyimide and the amine-functionalized MOF enhances the chemical stability and polymer chain rigidity. The hierarchical ZIF-8-NH2 MMMs exhibit a significantly improved gas permeability because of the accelerated molecular diffusion through the direction-oriented MOF pathway. For example, the ZIF-8-NH2 30 wt % MMM showed ∼6- and ∼4-fold enhanced H2 (761.7 Barrer) and CO2 (552.4 Barrer) permeabilities when compared to those of a pure polyimide film, with an H2/CH4 selectivity of 35.7 and CO2/CH4 selectivity of 25.9. Additionally, the MMM exhibits an improved plasticization resistance due to the connected MOF structure and MOF–polymer interaction. This strategy provides remarkable insight into the rational design of the polymer and MOF constituents in the MMM system.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsapm.2c00843
Chinese Library Classification Number:
Citation Information:
Herein, we report a facile approach to engineer a metal–organic framework (MOF) structure and polymer–MOF interface in a mixed-matrix membrane (MMM) to achieve high gas separation performance and plasticization resistance. Hierarchical ZIF-8-NH2 nanoparticles with a relatively small concentration of amine functionality (∼5 mol %) were prepared. The hierarchical MOF structure provides fast molecular transport pathways because of the MOF–MOF percolated network and high MOF packing density. Moreover, the interfacial interaction between the 6FDA-DAM:DABA(3:2) polyimide and the amine-functionalized MOF enhances the chemical stability and polymer chain rigidity. The hierarchical ZIF-8-NH2 MMMs exhibit a significantly improved gas permeability because of the accelerated molecular diffusion through the direction-oriented MOF pathway. For example, the ZIF-8-NH2 30 wt % MMM showed ∼6- and ∼4-fold enhanced H2 (761.7 Barrer) and CO2 (552.4 Barrer) permeabilities when compared to those of a pure polyimide film, with an H2/CH4 selectivity of 35.7 and CO2/CH4 selectivity of 25.9. Additionally, the MMM exhibits an improved plasticization resistance due to the connected MOF structure and MOF–polymer interaction. This strategy provides remarkable insight into the rational design of the polymer and MOF constituents in the MMM system.
quote
| GB/T 7714-2015 | [1] Jin Hui Jo, Chang Oh Lee, Gun Young Ryu, et al. ACS Applied Polymer Materials, 2022(4). DOI:10.1021/acsapm.2c00843. |
| MLA | [1] Jin Hui Jo, et al., ACS Applied Polymer Materials, no. 4, 2022, https://doi.org/10.1021/acsapm.2c00843. |
| APA | [1] Jin Hui Jo, Chang Oh Lee, Gun Young Ryu, Hyunmo Jae, Dongkyu Roh, & Won Seok Chi. (2022). ACS Applied Polymer Materials(4). https://doi.org/10.1021/acsapm.2c00843 |
| IEEE | [1] Jin Hui Jo, Chang Oh Lee, Gun Young Ryu, Hyunmo Jae, Dongkyu Roh, and Won Seok Chi, ACS Applied Polymer Materials, no. 4, 2022, doi: 10.1021/acsapm.2c00843. keywords: {ZIF8NH2;mixedmatrix membranes (MMMs);gas separation;hierarchical structure;interfacial interaction} |