Influence of Solvent Coordination on Hybrid Organic–Inorganic Perovskite Formation AITranslate
Abstract AITranslate
Solution-processed hybrid organic–inorganic perovskites (HOIPs) from organoammonium halide and lead halide precursors form efficacious active layers for photovoltaics, light-emitting diodes, and flexible electronics. Though solvent–solute coordination plays a critical role in HOIP crystallization, the influence of solvent choice on such interactions is poorly understood. We demonstrate Gutmann’s donor number, DN, as a parameter that indicates the coordinating ability of the processing solvent with the Pb2+ center of the lead halide precursor. Low DN solvents interact weakly with the Pb2+ center, favoring instead complexation between Pb2+ and iodide and subsequent crystallization of perovskite. High DN solvents coordinate more strongly with the Pb2+ center, which in turn inhibits iodide coordination and stalls perovskite crystallization. Varying the concentration of high-DN additives in precursor solutions tunes the strength of lead–solvent interactions, allowing finer control over the crystallization and the resulting morphology of HOIP active layers.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsenergylett.7b01057
Chinese Library Classification Number:
Citation Information:
Solution-processed hybrid organic–inorganic perovskites (HOIPs) from organoammonium halide and lead halide precursors form efficacious active layers for photovoltaics, light-emitting diodes, and flexible electronics. Though solvent–solute coordination plays a critical role in HOIP crystallization, the influence of solvent choice on such interactions is poorly understood. We demonstrate Gutmann’s donor number, DN, as a parameter that indicates the coordinating ability of the processing solvent with the Pb2+ center of the lead halide precursor. Low DN solvents interact weakly with the Pb2+ center, favoring instead complexation between Pb2+ and iodide and subsequent crystallization of perovskite. High DN solvents coordinate more strongly with the Pb2+ center, which in turn inhibits iodide coordination and stalls perovskite crystallization. Varying the concentration of high-DN additives in precursor solutions tunes the strength of lead–solvent interactions, allowing finer control over the crystallization and the resulting morphology of HOIP active layers.
quote
| GB/T 7714-2015 | [1] J. Clay Hamill, Jr., Jeffrey Schwartz, YuehLin Loo. ACS Energy Letters, 2018(3). DOI:10.1021/acsenergylett.7b01057. |
| MLA | [1] J. Clay Hamill, Jr., et al., ACS Energy Letters, no. 3, 2018, https://doi.org/10.1021/acsenergylett.7b01057. |
| APA | [1] J. Clay Hamill, Jr., Jeffrey Schwartz, & YuehLin Loo. (2018). ACS Energy Letters(3). https://doi.org/10.1021/acsenergylett.7b01057 |
| IEEE | [1] J. Clay Hamill, Jr., Jeffrey Schwartz, and YuehLin Loo, ACS Energy Letters, no. 3, 2018, doi: 10.1021/acsenergylett.7b01057. |