In Situ Engineering of Double-Phase Interface in Mo/Mo2C Heteronanosheets for Boosted Hydrogen Evolution Reaction AITranslate

China University of Geosciences (Wuhan)
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Two-dimensional Mo/Mo2C heteronanosheets (Mo/Mo2C-HNS) were successfully prepared via a NaCl template-assisted synthesis route followed by a controllable simultaneous reduction and carbonization of MoO3 nanosheets for efficient hydrogen evolution reaction (HER) catalysis under both acidic and alkaline conditions. The Mo species in the atomically thin Mo/Mo2C-HNS not only guarantees the rapid transport of electrons but also optimizes the electronic configuration of β-Mo2C. Besides, the abundant Mo/β-Mo2C heterointerfaces in nanodimension afford large numbers of additional heterogeneous catalytic sites. HER electrocatalytic performance with overpotential of merely 89 mV to drive a current density of 10 mA/cm2 in 0.5 M H2SO4 is therefore achieved. Strikingly, stable chronoamperometric electrolysis for 20 h and also an impressive cycling stability with negligible overpotential decay over 4000 sweeps demonstrate its considerable durability in an acidic environment. These findings highlight the promising potential of Mo/Mo2C-HNS catalyst as an efficient and stable noble metal-free electrocatalyst toward the HER.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.7b01180

Chinese Library Classification Number:

Citation Information:

Two-dimensional Mo/Mo2C heteronanosheets (Mo/Mo2C-HNS) were successfully prepared via a NaCl template-assisted synthesis route followed by a controllable simultaneous reduction and carbonization of MoO3 nanosheets for efficient hydrogen evolution reaction (HER) catalysis under both acidic and alkaline conditions. The Mo species in the atomically thin Mo/Mo2C-HNS not only guarantees the rapid transport of electrons but also optimizes the electronic configuration of β-Mo2C. Besides, the abundant Mo/β-Mo2C heterointerfaces in nanodimension afford large numbers of additional heterogeneous catalytic sites. HER electrocatalytic performance with overpotential of merely 89 mV to drive a current density of 10 mA/cm2 in 0.5 M H2SO4 is therefore achieved. Strikingly, stable chronoamperometric electrolysis for 20 h and also an impressive cycling stability with negligible overpotential decay over 4000 sweeps demonstrate its considerable durability in an acidic environment. These findings highlight the promising potential of Mo/Mo2C-HNS catalyst as an efficient and stable noble metal-free electrocatalyst toward the HER.

quote

GB/T 7714-2015 [1] Hansong Cheng. ACS Energy Letters, 2018(3). DOI:10.1021/acsenergylett.7b01180.
MLA [1] Hansong Cheng. ACS Energy Letters, no. 3, 2018, https://doi.org/10.1021/acsenergylett.7b01180.
APA [1] Hansong Cheng. (2018). ACS Energy Letters(3). https://doi.org/10.1021/acsenergylett.7b01180
IEEE [1] Hansong Cheng, ACS Energy Letters, no. 3, 2018, doi: 10.1021/acsenergylett.7b01180.