daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Multiple Cross-Linking-Dominated Metal–Ligand Coordinated Hydrogels with Tunable Strength and Thermosensitivity AITranslate

Shandong University; Shandong University; Shandong University; Shandong University; Shandong University; Shandong University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Development of stimuli-responsive hydrogels with improving mechanical strength is highly important for widening the practical applications of the smart soft hydrogel materials. In this paper, the metal–ligand coordinated hydrogels with tunable strength and thermosensitivity were fabricated by a facile two-step method including polymerization and post cross-linking. Compressive tests indicate that the covalent cross-linking degree, coordinated cross-linking degree and the type of coordinated metal ions largely impact the mechanical properties. Four types of the first transition metal ions including Zn2+, Cu2+, Co2+, and Ni2+ were used for coordination, which enhanced the mechanical properties of the hydrogels to different extents. In particular, the compressive strength of Zn2+ coordinated hydrogel is significantly improved compared with other ions coordinated hydrogels. The deswelling tests and differential scanning calorimetry (DSC) characterizations proved that the type of metal ions has great influence on the lower critical solution temperature (LCST) of the hydrogels. Herein, we attribute the different mechanical strength and phase transition behavior to the relaxation times as well as the divers spatial cross-linking density of the hydrogels, which may provide a avenue for the design of high-strength and fast-response hydrogels.

KeyWords AITranslate

hydrogels crosslinking metal−ligand coordination tunable strength tunable thermosensitivity
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.9b00490

Chinese Library Classification Number:

Citation Information:

Development of stimuli-responsive hydrogels with improving mechanical strength is highly important for widening the practical applications of the smart soft hydrogel materials. In this paper, the metal–ligand coordinated hydrogels with tunable strength and thermosensitivity were fabricated by a facile two-step method including polymerization and post cross-linking. Compressive tests indicate that the covalent cross-linking degree, coordinated cross-linking degree and the type of coordinated metal ions largely impact the mechanical properties. Four types of the first transition metal ions including Zn2+, Cu2+, Co2+, and Ni2+ were used for coordination, which enhanced the mechanical properties of the hydrogels to different extents. In particular, the compressive strength of Zn2+ coordinated hydrogel is significantly improved compared with other ions coordinated hydrogels. The deswelling tests and differential scanning calorimetry (DSC) characterizations proved that the type of metal ions has great influence on the lower critical solution temperature (LCST) of the hydrogels. Herein, we attribute the different mechanical strength and phase transition behavior to the relaxation times as well as the divers spatial cross-linking density of the hydrogels, which may provide a avenue for the design of high-strength and fast-response hydrogels.

quote

GB/T 7714-2015 [1] Yiyi Guo, Zhiliang Gao, Yihan Liu, et al. ACS Applied Polymer Materials, 2019(1). DOI:10.1021/acsapm.9b00490.
MLA [1] Yiyi Guo, et al., ACS Applied Polymer Materials, no. 1, 2019, https://doi.org/10.1021/acsapm.9b00490.
APA [1] Yiyi Guo, Zhiliang Gao, Yihan Liu, Zhaohui Huang, Chunxiao Chai, & Jingcheng Hao. (2019). ACS Applied Polymer Materials(1). https://doi.org/10.1021/acsapm.9b00490
IEEE [1] Yiyi Guo, Zhiliang Gao, Yihan Liu, Zhaohui Huang, Chunxiao Chai, and Jingcheng Hao, ACS Applied Polymer Materials, no. 1, 2019, doi: 10.1021/acsapm.9b00490. keywords: {hydrogels;crosslinking;metal−ligand coordination;tunable strength;tunable thermosensitivity}