Abstract AITranslate

Highlights • (5, 5), (10, 10) and (5, 5)@(10, 10) nanocoils have be constructed for MD simulation. • The maximum tensile strength and Young’s modulus of these nanocoils are obtained. • Slip vector is used to study the structural variations during the tension process in detail. • Nanocoils have not only a similar max stress with CNTs but also superelasticity. Molecular dynamics simulation was used to investigate the mechanical properties of (5, 5), and (10, 10) single-walled nanocoils, as well as (5, 5)@(10, 10) double-walled carbon nanocoils (CNCS). The second reactive empirical bond order potential was employed to model the interaction between carbon atoms. The atomic slip vector and sequential slip vector were used to investigate the structural variations at different strains during the tension process. The yield stress, maximum tensile strength, and Young’s modulus were determined from the tensile stress–strain profiles. The results show that the nanocoils have superelastic characteristics and have a high strength similar to that of carbon nanotube with same chirality.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1016/j.commatsci.2013.09.024

Chinese Library Classification Number:

Citation Information:

Highlights • (5, 5), (10, 10) and (5, 5)@(10, 10) nanocoils have be constructed for MD simulation. • The maximum tensile strength and Young’s modulus of these nanocoils are obtained. • Slip vector is used to study the structural variations during the tension process in detail. • Nanocoils have not only a similar max stress with CNTs but also superelasticity. Molecular dynamics simulation was used to investigate the mechanical properties of (5, 5), and (10, 10) single-walled nanocoils, as well as (5, 5)@(10, 10) double-walled carbon nanocoils (CNCS). The second reactive empirical bond order potential was employed to model the interaction between carbon atoms. The atomic slip vector and sequential slip vector were used to investigate the structural variations at different strains during the tension process. The yield stress, maximum tensile strength, and Young’s modulus were determined from the tensile stress–strain profiles. The results show that the nanocoils have superelastic characteristics and have a high strength similar to that of carbon nanotube with same chirality.

quote

GB/T 7714-2015 [1] ShinPon Ju, JennSen Lin, HuiLung Chen, et al. Computational Materials Science, 2014(82). DOI:10.1016/j.commatsci.2013.09.024.
MLA [1] ShinPon Ju, et al., Computational Materials Science, no. 82, 2014, https://doi.org/10.1016/j.commatsci.2013.09.024.
APA [1] ShinPon Ju, JennSen Lin, HuiLung Chen, JinYuan Hsieh, HsinTsung Chen, MengHsiung Weng, JiJun Zhao, LiZhao Liu, & MingChang Chen. (2014). Computational Materials Science(82). https://doi.org/10.1016/j.commatsci.2013.09.024
IEEE [1] ShinPon Ju, JennSen Lin, HuiLung Chen, JinYuan Hsieh, HsinTsung Chen, MengHsiung Weng, JiJun Zhao, LiZhao Liu, and MingChang Chen, Computational Materials Science, no. 82, 2014, doi: 10.1016/j.commatsci.2013.09.024.