Recent advances in the operando structural and interface characterisation of electrocatalysts AITranslate

The Hong Kong Polytechnic University; Shanghai Institute of Ceramics; The Hong Kong Polytechnic University; The Hong Kong Polytechnic University
AITranslate
Publisher: Elsevier
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Using multiple operando characterisation techniques to elucidate the structure-reactivity correlations of electrocatalytic systems is becoming more desirable. In this review article, we primarily employed the electrocatalytic CO2 reduction reaction over nanocatalysts as a model reaction to discuss the recent advances in the use of operando characterisation techniques. The synergy between various techniques can circumvent, to a great extent, the limitations of using one sole technique. For instance, the advances in using a combination of operando powder X-ray diffraction and Raman spectroscopy are discussed, which enables the complementary characterisation of nanocatalysts in both bulk and surface levels. Under operando conditions, the adsorbate and intermediate species, as well as the structural parameters of the catalyst can be simultaneously tracked for an extensive understanding of the reaction mechanisms.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1016/j.coelec.2023.101215

Chinese Library Classification Number:

Citation Information:

Using multiple operando characterisation techniques to elucidate the structure-reactivity correlations of electrocatalytic systems is becoming more desirable. In this review article, we primarily employed the electrocatalytic CO2 reduction reaction over nanocatalysts as a model reaction to discuss the recent advances in the use of operando characterisation techniques. The synergy between various techniques can circumvent, to a great extent, the limitations of using one sole technique. For instance, the advances in using a combination of operando powder X-ray diffraction and Raman spectroscopy are discussed, which enables the complementary characterisation of nanocatalysts in both bulk and surface levels. Under operando conditions, the adsorbate and intermediate species, as well as the structural parameters of the catalyst can be simultaneously tracked for an extensive understanding of the reaction mechanisms.

quote

GB/T 7714-2015 [1] Hao Zhang, Zhengyang Zhou, Qiong Lei, et al. Current Opinion in Electrochemistry, 2023(38). DOI:10.1016/j.coelec.2023.101215.
MLA [1] Hao Zhang, et al., Current Opinion in Electrochemistry, no. 38, 2023, https://doi.org/10.1016/j.coelec.2023.101215.
APA [1] Hao Zhang, Zhengyang Zhou, Qiong Lei, & Tsz Woon Benedict Lo. (2023). Current Opinion in Electrochemistry(38). https://doi.org/10.1016/j.coelec.2023.101215
IEEE [1] Hao Zhang, Zhengyang Zhou, Qiong Lei, and Tsz Woon Benedict Lo, Current Opinion in Electrochemistry, no. 38, 2023, doi: 10.1016/j.coelec.2023.101215.