Green Emitting Single-Crystalline Bulk Assembly of Metal Halide Clusters with Near-Unity Photoluminescence Quantum Efficiency AITranslate
Abstract AITranslate
Organic metal halide hybrids with zero-dimensional (0D) structure at the molecular level, or single-crystalline bulk assemblies of metal halides, are an emerging class of light-emitting materials with high photoluminescence quantum efficiencies (PLQEs) and color tunability. Here we report the synthesis and characterization of a new single-crystalline bulk assembly of metal halide clusters, (bmpy)9[ZnCl4]2[Pb3Cl11] (bmpy: 1-butyl-1-methylpyrrolidinium), which exhibits green emission peaked at 512 nm with a remarkable near-unity PLQE at room temperature. Detailed structural and photophysical studies suggest that there are two emitting states in [Pb3Cl11]5– clusters, whose populations are strongly dependent on the surrounding molecular environment that controls the excited-state structural distortion of [Pb3Cl11]5– clusters. High chemical- and photostability have also been demonstrated in this new material.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsenergylett.9b00991
Chinese Library Classification Number:
Citation Information:
Organic metal halide hybrids with zero-dimensional (0D) structure at the molecular level, or single-crystalline bulk assemblies of metal halides, are an emerging class of light-emitting materials with high photoluminescence quantum efficiencies (PLQEs) and color tunability. Here we report the synthesis and characterization of a new single-crystalline bulk assembly of metal halide clusters, (bmpy)9[ZnCl4]2[Pb3Cl11] (bmpy: 1-butyl-1-methylpyrrolidinium), which exhibits green emission peaked at 512 nm with a remarkable near-unity PLQE at room temperature. Detailed structural and photophysical studies suggest that there are two emitting states in [Pb3Cl11]5– clusters, whose populations are strongly dependent on the surrounding molecular environment that controls the excited-state structural distortion of [Pb3Cl11]5– clusters. High chemical- and photostability have also been demonstrated in this new material.
quote
| GB/T 7714-2015 | [1] Chenkun Zhou, Haoran Lin, Jennifer Neu, et al. ACS Energy Letters, 2019(4). DOI:10.1021/acsenergylett.9b00991. |
| MLA | [1] Chenkun Zhou, et al., ACS Energy Letters, no. 4, 2019, https://doi.org/10.1021/acsenergylett.9b00991. |
| APA | [1] Chenkun Zhou, Haoran Lin, Jennifer Neu, Yan Zhou, Maya Chaaban, Sujin Lee, Michael Worku, Banghao Chen, Ronald Clark, Wenhao Cheng, Jingjiao Guan, Peter Djurovich, Dongzhou Zhang, Xujie Lü, James Bullock, Chongin Pak, Michael Shatruk, MaoHua Du, Theo Siegrist, & Biwu Ma. (2019). ACS Energy Letters(4). https://doi.org/10.1021/acsenergylett.9b00991 |
| IEEE | [1] Chenkun Zhou, Haoran Lin, Jennifer Neu, Yan Zhou, Maya Chaaban, Sujin Lee, Michael Worku, Banghao Chen, Ronald Clark, Wenhao Cheng, Jingjiao Guan, Peter Djurovich, Dongzhou Zhang, Xujie Lü, James Bullock, Chongin Pak, Michael Shatruk, MaoHua Du, Theo Siegrist, and Biwu Ma, ACS Energy Letters, no. 4, 2019, doi: 10.1021/acsenergylett.9b00991. |