daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Semiaromatic Polyesters from a Rigid Diphenyl-Terephthalic Acid: From Synthesis to Properties AITranslate

Tianjin University of Technology; Tianjin University of Technology; Tianjin University of Technology; Tianjin University of Technology;Jiangsu Guowang High-Technique Fiber Co.; Tianjin University of Technology
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Semiaromatic polyesters with a high glass transition temperature (Tg) are promising materials in demanding fields. Herein, a highly rigid diester, diethyl-2,3-diphenyl-1,4-benzenedicarboxylate (DDB), was synthesized from naturally occurring citric acid and cinnamaldehyde. DDB was used to synthesize a series of biobased polyesters by melt polymerization with linear and cyclic diols. Single-crystal X-ray diffraction analysis revealed that DDB crystallized in the monoclinic crystal system with the pendant phenyl groups almost orthogonal to the central benzene ring. The DDB polyesters based on alkanediols (abbreviated as PD-ms) exhibited high number average molecular weights (Mn) in the range of 10,700–39,800 g mol–1. Thermogravimetric analysis (TGA) demonstrated their excellent thermostability that was comparable to petroleum-based polyesters. The crystallization of the PD-ms series was partially caused due to the π–π stacking of DDB units. The DDB homopolyester based on 1,10-decanediol showed a combination of high modulus, high tensile strength, and high ductility of 762, 17 MPa, and 153%, respectively. This was achieved due to the synergistic effects of the rigid DDB and the flexible 1,10-decanediol units. Lastly, DDB imparted inherent UV-blocking properties to polymers, which made them applicable in UV-protective and transparent films. In view of the fertile chemistry of biobased aromatic aldehydes, this work paves a path to DDB derivatives that are attractive precursors for semiaromatic polyesters.

KeyWords AITranslate

renewable highTg polyester citric acid cinnamaldehyde
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.2c02101

Chinese Library Classification Number:

Citation Information:

Semiaromatic polyesters with a high glass transition temperature (Tg) are promising materials in demanding fields. Herein, a highly rigid diester, diethyl-2,3-diphenyl-1,4-benzenedicarboxylate (DDB), was synthesized from naturally occurring citric acid and cinnamaldehyde. DDB was used to synthesize a series of biobased polyesters by melt polymerization with linear and cyclic diols. Single-crystal X-ray diffraction analysis revealed that DDB crystallized in the monoclinic crystal system with the pendant phenyl groups almost orthogonal to the central benzene ring. The DDB polyesters based on alkanediols (abbreviated as PD-ms) exhibited high number average molecular weights (Mn) in the range of 10,700–39,800 g mol–1. Thermogravimetric analysis (TGA) demonstrated their excellent thermostability that was comparable to petroleum-based polyesters. The crystallization of the PD-ms series was partially caused due to the π–π stacking of DDB units. The DDB homopolyester based on 1,10-decanediol showed a combination of high modulus, high tensile strength, and high ductility of 762, 17 MPa, and 153%, respectively. This was achieved due to the synergistic effects of the rigid DDB and the flexible 1,10-decanediol units. Lastly, DDB imparted inherent UV-blocking properties to polymers, which made them applicable in UV-protective and transparent films. In view of the fertile chemistry of biobased aromatic aldehydes, this work paves a path to DDB derivatives that are attractive precursors for semiaromatic polyesters.

quote

GB/T 7714-2015 [1] Shengke Zhao, Jie Zhang, Xiaoyu Wang, et al. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.2c02101.
MLA [1] Shengke Zhao, et al., ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.2c02101.
APA [1] Shengke Zhao, Jie Zhang, Xiaoyu Wang, Lin Wang, Jia Wang, & Chengcai Pang. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.2c02101
IEEE [1] Shengke Zhao, Jie Zhang, Xiaoyu Wang, Lin Wang, Jia Wang, and Chengcai Pang, ACS Applied Polymer Materials, no. 5, 2023, doi: 10.1021/acsapm.2c02101. keywords: {renewable;highTg;polyester;citric acid;cinnamaldehyde}