Simple Fabrication of PDMS-Grafted Hydrophobic Iron Oxide Particles for Oil–Water Separation and Stimuli-Responsive Liquid Marbles AITranslate

Department of Atomic and Molecular Physics, Manipal Academy of Higher Education; National Institute of Technology Calicut; National Institute of Technology Calicut;Department of Atomic and Molecular Physics, Manipal Academy of Higher Education
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

In this paper, poly(dimethyl siloxane) (PDMS) which is considered chemically unreactive was successfully grafted onto the surface of iron oxide particles, forming stable hydrophobic polymer-coated particles without the usage of any external stimuli like heat or UV irradiation. Here, magnetic hydrophobic particles were prepared by a facile method of coating PDMS prepolymer oil onto Fe3O4 particles via dispersion in a PDMS oil/hexane solution. The X-ray diffraction studies elucidated the successful synthesis of the magnetic particles, whereas the X-ray photoelectron spectroscopic studies ensure the successful incorporation of the polymer layer onto the particles. Two potential applications of the prepared particles were demonstrated here. The oleophilic and hydrophobic nature of the particles coated with PDMS is exploited to demonstrate the oil collection from the surface as well as in immersed conditions in an aqueous medium by using the particle-coated cotton and sponge, respectively. An oil–water separation efficiency of ∼95% was achieved for cotton and sponge against various oils with an oil adsorption capacity of 5 times and 11 times its own weight, respectively. Additionally, magnetic-responsive liquid marbles (LMs) were prepared by encapsulating liquids with the fabricated particles. Stable LMs were formed for a wide range of volumes (5–200 μL) with core liquids having different surface tensions, pH, and viscosity. The stability of the LM was tested using a dropping method and a hydrostatic pressure method.

KeyWords AITranslate

polydimethylsiloxane coating magnetic liquid marble oil−water separation hydrophobic particles polymer grafting Show More
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.3c00186

Chinese Library Classification Number:

Citation Information:

In this paper, poly(dimethyl siloxane) (PDMS) which is considered chemically unreactive was successfully grafted onto the surface of iron oxide particles, forming stable hydrophobic polymer-coated particles without the usage of any external stimuli like heat or UV irradiation. Here, magnetic hydrophobic particles were prepared by a facile method of coating PDMS prepolymer oil onto Fe3O4 particles via dispersion in a PDMS oil/hexane solution. The X-ray diffraction studies elucidated the successful synthesis of the magnetic particles, whereas the X-ray photoelectron spectroscopic studies ensure the successful incorporation of the polymer layer onto the particles. Two potential applications of the prepared particles were demonstrated here. The oleophilic and hydrophobic nature of the particles coated with PDMS is exploited to demonstrate the oil collection from the surface as well as in immersed conditions in an aqueous medium by using the particle-coated cotton and sponge, respectively. An oil–water separation efficiency of ∼95% was achieved for cotton and sponge against various oils with an oil adsorption capacity of 5 times and 11 times its own weight, respectively. Additionally, magnetic-responsive liquid marbles (LMs) were prepared by encapsulating liquids with the fabricated particles. Stable LMs were formed for a wide range of volumes (5–200 μL) with core liquids having different surface tensions, pH, and viscosity. The stability of the LM was tested using a dropping method and a hydrostatic pressure method.

quote

GB/T 7714-2015 [1] Swithin Hanosh, Bindhu Sunilkumar Lekshmi, Subramanyan Namboodiri Varanakkottu, et al. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.3c00186.
MLA [1] Swithin Hanosh, et al., ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.3c00186.
APA [1] Swithin Hanosh, Bindhu Sunilkumar Lekshmi, Subramanyan Namboodiri Varanakkottu, & Sajan D. George. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.3c00186
IEEE [1] Swithin Hanosh, Bindhu Sunilkumar Lekshmi, Subramanyan Namboodiri Varanakkottu, and Sajan D. George, ACS Applied Polymer Materials, no. 5, 2023, doi: 10.1021/acsapm.3c00186. keywords: {polydimethylsiloxane coating;magnetic liquid marble;oil−water separation;hydrophobic particles;polymer grafting;Show More}