Atomically thin 2D van der Waals (2D-vDW) materials have attracted significant attention for optoelectronic applications in photodetectors, photovoltaics, and quantum information science. Their atomically thin thickness, however, renders them poor absorbers. Hybrid structures of 2D-vDW materials assembled with other semiconducting materials, such as quantum dots, nanowires, polymers, other 2D-vDW materials, or 3D bulk materials, have provided an elegant way to increase light harvesting and carrier generation via interfacial charge and energy transfer interactions. Here we present recent examples focused on the characterization of interfacial charge transfer and energy transfer in 2D-vDW hybrids and heterostructures and methods to modulate and control these processes through band gap engineering, morphology engineering, and external factors. Finally, we discuss potential future directions of research, including scalability from micron-sized flake-based devices to wafer size for commercial deployment, issues with long-term stability and performance, and the ability to extend the spectral range of these 2D hybrids.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.9b01399

Chinese Library Classification Number:

Citation Information:

Atomically thin 2D van der Waals (2D-vDW) materials have attracted significant attention for optoelectronic applications in photodetectors, photovoltaics, and quantum information science. Their atomically thin thickness, however, renders them poor absorbers. Hybrid structures of 2D-vDW materials assembled with other semiconducting materials, such as quantum dots, nanowires, polymers, other 2D-vDW materials, or 3D bulk materials, have provided an elegant way to increase light harvesting and carrier generation via interfacial charge and energy transfer interactions. Here we present recent examples focused on the characterization of interfacial charge transfer and energy transfer in 2D-vDW hybrids and heterostructures and methods to modulate and control these processes through band gap engineering, morphology engineering, and external factors. Finally, we discuss potential future directions of research, including scalability from micron-sized flake-based devices to wafer size for commercial deployment, issues with long-term stability and performance, and the ability to extend the spectral range of these 2D hybrids.

quote

GB/T 7714-2015 [1] Mingxing Li, JiaShiang Chen, Mircea Cotlet. ACS Energy Letters, 2019(4). DOI:10.1021/acsenergylett.9b01399.
MLA [1] Mingxing Li, et al., ACS Energy Letters, no. 4, 2019, https://doi.org/10.1021/acsenergylett.9b01399.
APA [1] Mingxing Li, JiaShiang Chen, & Mircea Cotlet. (2019). ACS Energy Letters(4). https://doi.org/10.1021/acsenergylett.9b01399
IEEE [1] Mingxing Li, JiaShiang Chen, and Mircea Cotlet, ACS Energy Letters, no. 4, 2019, doi: 10.1021/acsenergylett.9b01399.