New Insight on the Role of Electrolyte Additives in Rechargeable Lithium Ion Batteries AITranslate

King Abdullah University of Science and Technology (KAUST); King Abdullah University of Science and Technology (KAUST); King Abdullah University of Science and Technology (KAUST); King Abdullah University of Science and Technology (KAUST); King Abdullah University of Science and Technology (KAUST); King Abdullah University of Science and Technology (KAUST); King Abdullah University of Science and Technology (KAUST); Hanyang University; Changchun Institute of Applied Chemistry; King Abdullah University of Science and Technology (KAUST); Hanyang University; King Abdullah University of Science and Technology (KAUST)
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Solid electrolyte interphase (SEI)-forming agents such as vinylene carbonate, sulfone, and cyclic sulfate are commonly believed to be film-forming additives in lithium-ion batteries that help to enhance graphite anode stability. However, we find that the film-forming effect and the resultant SEI may not be the only reasons for the enhanced graphite stability. This is because the as-formed SEI cannot inhibit Li+–solvent co-intercalation once the additive is removed from the electrolyte. Instead, we show that the Li+ solvation structure, which is modified by these additives, plays a critical role in achieving reversible Li+ (de)intercalation within graphite. This discovery is confirmed in both carbonate and ether-based electrolytes. We show that the problem of graphite exfoliation caused by Li+–solvent co-intercalation can be mitigated by adding ethene sulfate to tune the Li+ coordination structure. This work brings new insight into the role of additives in electrolytes, expanding the prevailing thinking over the past 2 decades. In addition, this finding can guide the design of more versatile electrolytes for advanced rechargeable metal-ion batteries.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.9b01441

Chinese Library Classification Number:

Citation Information:

Solid electrolyte interphase (SEI)-forming agents such as vinylene carbonate, sulfone, and cyclic sulfate are commonly believed to be film-forming additives in lithium-ion batteries that help to enhance graphite anode stability. However, we find that the film-forming effect and the resultant SEI may not be the only reasons for the enhanced graphite stability. This is because the as-formed SEI cannot inhibit Li+–solvent co-intercalation once the additive is removed from the electrolyte. Instead, we show that the Li+ solvation structure, which is modified by these additives, plays a critical role in achieving reversible Li+ (de)intercalation within graphite. This discovery is confirmed in both carbonate and ether-based electrolytes. We show that the problem of graphite exfoliation caused by Li+–solvent co-intercalation can be mitigated by adding ethene sulfate to tune the Li+ coordination structure. This work brings new insight into the role of additives in electrolytes, expanding the prevailing thinking over the past 2 decades. In addition, this finding can guide the design of more versatile electrolytes for advanced rechargeable metal-ion batteries.

quote

GB/T 7714-2015 [1] Jun Ming, Zhen Cao, Yingqiang Wu, et al. ACS Energy Letters, 2019(4). DOI:10.1021/acsenergylett.9b01441.
MLA [1] Jun Ming, et al., ACS Energy Letters, no. 4, 2019, https://doi.org/10.1021/acsenergylett.9b01441.
APA [1] Jun Ming, Zhen Cao, Yingqiang Wu, Wandi Wahyudi, Wenxi Wang, Xianrong Guo, Luigi Cavallo, JangYeon Hwang, Atif Shamim, LainJong Li, YangKook Sun, & Husam N. Alshareef. (2019). ACS Energy Letters(4). https://doi.org/10.1021/acsenergylett.9b01441
IEEE [1] Jun Ming, Zhen Cao, Yingqiang Wu, Wandi Wahyudi, Wenxi Wang, Xianrong Guo, Luigi Cavallo, JangYeon Hwang, Atif Shamim, LainJong Li, YangKook Sun, and Husam N. Alshareef, ACS Energy Letters, no. 4, 2019, doi: 10.1021/acsenergylett.9b01441.