Biobased Polyester Network from 2,5-Furandicarboxylic Acid and 5,5′-((Dodecylazanediyl)bis(methylene))bis(furan-5,2-diyl))dimethanol: Shape Memory, Adhesiveness, Self-Healing, and Recyclability AITranslate

Southwest Petroleum University; Dalian Institute of Chemical Physics; Dalian Institute of Chemical Physics; Southwest Petroleum University; Dalian Institute of Chemical Physics; Dalian Institute of Chemical Physics
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The preparation of recyclable multifunctional biobased cross-linked polymers for different application environments and reducing dependence on petroleum products are important for sustainable development. Herein, we successfully synthesized a series of environmentally friendly, shape memory, adhesion, self-healing, and recyclable biobased polyester networks using 2,5-furandicarboxylic acid (FDCA) and 5,5′-((dodecylazanediyl)bis(methylene))bis(furan-5,2-diyl))dimethanol (DoDM) derived from renewable materials by introducing reversible Diels–Alder bonds with the addition of bismaleimide (BMI). Profiting from the freely rotating difuran ring group in DoDM, the cross-linked network with tunable thermal and mechanical properties can be constructed and present fascinating versatility. A kinetic analysis suggests that the reaction follows second-order kinetics, and the calculated activation energy is 48.1 kJ/mol with an optimal temperature of 60 °C. Different cross-linking densities of PDoF/BMI networks result in glass transition temperatures varying from 19 to 47 °C, tensile moduli from 22 to 529 MPa, and elongations at break from 5 to 120%. The PDoF/BMI network has a good shape memory performance: it can be fixed to a temporary shape below Tg and restored to its original shape by heating above Tg, with a shape recovery rate of up to 98%. In addition, the PDoF/BMI 10:1 polymer network can be used as a solvent-free adhesive with strong adhesion to glass (3.1 ± 0.5 kPa). The dynamic bond provides a self-healing response that can repair the surface scratch damage and contribute to 87% of the tensile stress recovery. Meanwhile, the PDoF/BMI film can be recovered after shredding, implying the good recyclability of the PDoF/BMI polymer. Therefore, the PDoF/BMI polymer, as a biobased multifunctional environmentally friendly material, has potential application prospects in a wide range of practical fields.

KeyWords AITranslate

biobased thermosets selfhealing properties recycling shape memory polymer adhesiveness of polymers
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.3c01427

Chinese Library Classification Number:

Citation Information:

The preparation of recyclable multifunctional biobased cross-linked polymers for different application environments and reducing dependence on petroleum products are important for sustainable development. Herein, we successfully synthesized a series of environmentally friendly, shape memory, adhesion, self-healing, and recyclable biobased polyester networks using 2,5-furandicarboxylic acid (FDCA) and 5,5′-((dodecylazanediyl)bis(methylene))bis(furan-5,2-diyl))dimethanol (DoDM) derived from renewable materials by introducing reversible Diels–Alder bonds with the addition of bismaleimide (BMI). Profiting from the freely rotating difuran ring group in DoDM, the cross-linked network with tunable thermal and mechanical properties can be constructed and present fascinating versatility. A kinetic analysis suggests that the reaction follows second-order kinetics, and the calculated activation energy is 48.1 kJ/mol with an optimal temperature of 60 °C. Different cross-linking densities of PDoF/BMI networks result in glass transition temperatures varying from 19 to 47 °C, tensile moduli from 22 to 529 MPa, and elongations at break from 5 to 120%. The PDoF/BMI network has a good shape memory performance: it can be fixed to a temporary shape below Tg and restored to its original shape by heating above Tg, with a shape recovery rate of up to 98%. In addition, the PDoF/BMI 10:1 polymer network can be used as a solvent-free adhesive with strong adhesion to glass (3.1 ± 0.5 kPa). The dynamic bond provides a self-healing response that can repair the surface scratch damage and contribute to 87% of the tensile stress recovery. Meanwhile, the PDoF/BMI film can be recovered after shredding, implying the good recyclability of the PDoF/BMI polymer. Therefore, the PDoF/BMI polymer, as a biobased multifunctional environmentally friendly material, has potential application prospects in a wide range of practical fields.

quote

GB/T 7714-2015 [1] Jing Yi, Yuze Dai, Yuxuan Li, et al. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.3c01427.
MLA [1] Jing Yi, et al., ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.3c01427.
APA [1] Jing Yi, Yuze Dai, Yuxuan Li, Yuanpeng Wu, Min Jiang, & Guangyuan Zhou. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.3c01427
IEEE [1] Jing Yi, Yuze Dai, Yuxuan Li, Yuanpeng Wu, Min Jiang, and Guangyuan Zhou, ACS Applied Polymer Materials, no. 5, 2023, doi: 10.1021/acsapm.3c01427. keywords: {biobased thermosets;selfhealing properties;recycling;shape memory polymer;adhesiveness of polymers}