daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Tuning Backbone Planarity in Thiadiazolobenzotriazole–Bis(thienothiophenyl)ethylene Copolymers for Organic Field-Effect Transistors AITranslate

Tokyo Institute of Technology; Tokyo Institute of Technology; Tokyo Institute of Technology; Tokyo Institute of Technology; Tokyo Institute of Technology; Tokyo Institute of Technology
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

[1,2,5]Thiadiazolo[3,4-f]benzotriazole (TBZ) and bis(thieno[3,2-b]thiophenyl)ethylene (DTTE)-based conjugated polymers were designed and synthesized by Stille polycondensation, and the effect of the side chain alkyl positions on the optical, electrochemical, and charge-transporting properties in organic field-effect transistors was comprehensively studied. By optimizing the alkyl positions, we obtained semicrystalline polymers, but their hole mobilities were ∼0.1 cm2 V–1 s–1 due to the face-on dominant orientation. It was also found that the thiophene spacers, which have traditionally been present in the TBZ-based copolymers, are the source of the backbone torsion. Removal of the thiophene units produced an almost planar copolymer backbone with an edge-on and bimodal texture, which exhibited the improved hole mobility exceeding 0.4 cm2 V–1 s–1.

KeyWords AITranslate

crystallinity organic transistors polycondensation semiconducting polymers structure−property relationship
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.9b00329

Chinese Library Classification Number:

Citation Information:

[1,2,5]Thiadiazolo[3,4-f]benzotriazole (TBZ) and bis(thieno[3,2-b]thiophenyl)ethylene (DTTE)-based conjugated polymers were designed and synthesized by Stille polycondensation, and the effect of the side chain alkyl positions on the optical, electrochemical, and charge-transporting properties in organic field-effect transistors was comprehensively studied. By optimizing the alkyl positions, we obtained semicrystalline polymers, but their hole mobilities were ∼0.1 cm2 V–1 s–1 due to the face-on dominant orientation. It was also found that the thiophene spacers, which have traditionally been present in the TBZ-based copolymers, are the source of the backbone torsion. Removal of the thiophene units produced an almost planar copolymer backbone with an edge-on and bimodal texture, which exhibited the improved hole mobility exceeding 0.4 cm2 V–1 s–1.

quote

GB/T 7714-2015 [1] Sultan Otep, Yang Wang, Akihiro Kohara, et al. ACS Applied Polymer Materials, 2019(1). DOI:10.1021/acsapm.9b00329.
MLA [1] Sultan Otep, et al., ACS Applied Polymer Materials, no. 1, 2019, https://doi.org/10.1021/acsapm.9b00329.
APA [1] Sultan Otep, Yang Wang, Akihiro Kohara, Hidetoshi Matsumoto, Takehiko Mori, & Tsuyoshi Michinobu. (2019). ACS Applied Polymer Materials(1). https://doi.org/10.1021/acsapm.9b00329
IEEE [1] Sultan Otep, Yang Wang, Akihiro Kohara, Hidetoshi Matsumoto, Takehiko Mori, and Tsuyoshi Michinobu, ACS Applied Polymer Materials, no. 1, 2019, doi: 10.1021/acsapm.9b00329. keywords: {crystallinity;organic transistors;polycondensation;semiconducting polymers;structure−property relationship}