Vanillin- and Isovanillin-Based Phthalonitrile Resins Containing Spirocycle Acetal Structures AITranslate

Beijing University of Chemical Technology; Beijing University of Chemical Technology; Beijing University of Chemical Technology; Beijing University of Chemical Technology;Beijing University of Chemical Technology;SINOPEC Beijing Research Institute of Chemical Industry;SINOPEC Beijing Research Institute of Chemical Industry; Beijing University of Chemical Technology
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Preparing biobased high-performance thermosetting resins is one of the most important factors for sustainable development. In this work, two kinds of phthalonitrile resins containing spirocycle acetal structures were synthesized from pentaerythritol and renewable vanillin and isovanillin by an efficient two-step process. The structures of vanillin- and isovanillin-based phthalonitrile (VPN and IVPN) monomers were characterized by Fourier transform infrared (FTIR), NMR, matrix-assisted laser desorption/ionization time-of-flight mass spectrometry, and elemental analysis. The curing behaviors of these monomers were studied by differential scanning calorimetry and FTIR. The thermal stability and dynamic mechanical properties of the cured resins were investigated by thermogravimetric analysis and dynamic mechanical thermal analysis. The processing properties were studied by a rheological analysis. Compared with traditional petroleum-based phthalonitrile resins such as bisphenol A and bisphenol, cured VPN and IVPN resins exhibited good thermal stability and thermomechanical properties, high glass transition temperature (Tg), and excellent processability.

KeyWords AITranslate

biobased spirocycle acetal phthalonitrile thermosets thermal stability
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.3c01138

Chinese Library Classification Number:

Citation Information:

Preparing biobased high-performance thermosetting resins is one of the most important factors for sustainable development. In this work, two kinds of phthalonitrile resins containing spirocycle acetal structures were synthesized from pentaerythritol and renewable vanillin and isovanillin by an efficient two-step process. The structures of vanillin- and isovanillin-based phthalonitrile (VPN and IVPN) monomers were characterized by Fourier transform infrared (FTIR), NMR, matrix-assisted laser desorption/ionization time-of-flight mass spectrometry, and elemental analysis. The curing behaviors of these monomers were studied by differential scanning calorimetry and FTIR. The thermal stability and dynamic mechanical properties of the cured resins were investigated by thermogravimetric analysis and dynamic mechanical thermal analysis. The processing properties were studied by a rheological analysis. Compared with traditional petroleum-based phthalonitrile resins such as bisphenol A and bisphenol, cured VPN and IVPN resins exhibited good thermal stability and thermomechanical properties, high glass transition temperature (Tg), and excellent processability.

quote

GB/T 7714-2015 [1] Ke Li, Xiaoyi Sun, Hua Yin, et al. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.3c01138.
MLA [1] Ke Li, et al., ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.3c01138.
APA [1] Ke Li, Xiaoyi Sun, Hua Yin, Kun Yang, Pei Dai, Ling Han, Longgui Zhang, & Riwei Xu. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.3c01138
IEEE [1] Ke Li, Xiaoyi Sun, Hua Yin, Kun Yang, Pei Dai, Ling Han, Longgui Zhang, and Riwei Xu, ACS Applied Polymer Materials, no. 5, 2023, doi: 10.1021/acsapm.3c01138. keywords: {biobased;spirocycle acetal;phthalonitrile;thermosets;thermal stability}