In this work, we demonstrate the successful application of two-dimensional (2D) materials, i.e., graphene and functionalized MoS2, in perovskite solar cells (PSCs) by interface engineering the standard mesoscopic n–i–p structure. The use of 2D materials has the dual role to improve both the stability and the overall power conversion efficiency (PCE) of the PSCs compared to standard devices. The application of 2D materials is successfully extended to large-area perovskite solar modules (PSMs), achieving PCEs of 13.4% and 15.3% on active areas of 108 cm2 and 82 cm2, respectively. This performance results in record-high active area-indexed aperture PCE (AIAPCE) of 1266.5% cm2. In addition, the 2D materials-based PSMs show a stability under a prolonged (>1000 h) thermal stress test at 65 °C (ISOS-D2), representing a crucial advancement in the exploitation of perovskite photovoltaic technology.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsenergylett.9b01151
Chinese Library Classification Number:
Citation Information:
In this work, we demonstrate the successful application of two-dimensional (2D) materials, i.e., graphene and functionalized MoS2, in perovskite solar cells (PSCs) by interface engineering the standard mesoscopic n–i–p structure. The use of 2D materials has the dual role to improve both the stability and the overall power conversion efficiency (PCE) of the PSCs compared to standard devices. The application of 2D materials is successfully extended to large-area perovskite solar modules (PSMs), achieving PCEs of 13.4% and 15.3% on active areas of 108 cm2 and 82 cm2, respectively. This performance results in record-high active area-indexed aperture PCE (AIAPCE) of 1266.5% cm2. In addition, the 2D materials-based PSMs show a stability under a prolonged (>1000 h) thermal stress test at 65 °C (ISOS-D2), representing a crucial advancement in the exploitation of perovskite photovoltaic technology.
quote
| GB/T 7714-2015 | [1] Antonio Agresti, Sara Pescetelli, Alessandro Lorenzo Palma, et al. ACS Energy Letters, 2019(4). DOI:10.1021/acsenergylett.9b01151. |
| MLA | [1] Antonio Agresti, et al., ACS Energy Letters, no. 4, 2019, https://doi.org/10.1021/acsenergylett.9b01151. |
| APA | [1] Antonio Agresti, Sara Pescetelli, Alessandro Lorenzo Palma, Beatriz MartínGarcía, Leyla Najafi, Sebastiano Bellani, Iwan Moreels, Mirko Prato, Francesco Bonaccorso, & Aldo Di Carlo. (2019). ACS Energy Letters(4). https://doi.org/10.1021/acsenergylett.9b01151 |
| IEEE | [1] Antonio Agresti, Sara Pescetelli, Alessandro Lorenzo Palma, Beatriz MartínGarcía, Leyla Najafi, Sebastiano Bellani, Iwan Moreels, Mirko Prato, Francesco Bonaccorso, and Aldo Di Carlo, ACS Energy Letters, no. 4, 2019, doi: 10.1021/acsenergylett.9b01151. |