Biofouling caused by nonspecific adsorption of biomolecules and organisms such as proteins, cells, and bacteria to material surfaces is a significant challenge for numerous important applications. An effective approach to addressing this problem is to coat antifouling polymers on the material surfaces to impart the demanded antifouling properties and repel nonspecific biological adhesion. In this review, we summarized recent advances in surface antifouling polymer brushes which have emerged in the past decade, with a focus on the origin of antifouling properties of polymer brushes, approaches to surface antifouling polymer brushes, key factors that impact antifouling properties, common antifouling polymers used for the construction of surface polymer brushes, and applications of antifouling polymer brushes in a variety of fields.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsapm.3c02150
Chinese Library Classification Number:
Citation Information:
Biofouling caused by nonspecific adsorption of biomolecules and organisms such as proteins, cells, and bacteria to material surfaces is a significant challenge for numerous important applications. An effective approach to addressing this problem is to coat antifouling polymers on the material surfaces to impart the demanded antifouling properties and repel nonspecific biological adhesion. In this review, we summarized recent advances in surface antifouling polymer brushes which have emerged in the past decade, with a focus on the origin of antifouling properties of polymer brushes, approaches to surface antifouling polymer brushes, key factors that impact antifouling properties, common antifouling polymers used for the construction of surface polymer brushes, and applications of antifouling polymer brushes in a variety of fields.
quote
| GB/T 7714-2015 | [1] Xin Xu, Yixin Chang, Yutong Gong, et al. ACS Applied Polymer Materials, 2024(6). DOI:10.1021/acsapm.3c02150. |
| MLA | [1] Xin Xu, et al., ACS Applied Polymer Materials, no. 6, 2024, https://doi.org/10.1021/acsapm.3c02150. |
| APA | [1] Xin Xu, Yixin Chang, Yutong Gong, Yuhao Zhang, Ye Yu, Hui Peng, & Changkui Fu. (2024). ACS Applied Polymer Materials(6). https://doi.org/10.1021/acsapm.3c02150 |
| IEEE | [1] Xin Xu, Yixin Chang, Yutong Gong, Yuhao Zhang, Ye Yu, Hui Peng, and Changkui Fu, ACS Applied Polymer Materials, no. 6, 2024, doi: 10.1021/acsapm.3c02150. keywords: {antifouling polymers;surface polymer brushes;synthesis approaches;molecular architectures;applications} |