Implicit scheme of RVE calculation for FCC polycrystals AITranslate
Abstract AITranslate
Considering the coupling effect between the nodal force equilibrium and internal variables evolution, an implicit scheme of solving the non-linear FEM problem is presented to modelling the texture evolution and the anisotropic behaviour of polycrystals for large deformation. This algorithm is based on the isomorphism theory that the current elastic law can be achieved through transferring the reference elastic law by a plastic transformation. Different time steps have been adopted with respect to the global and local iteration systems and the consistent tangent module is also calculated to construct a high speed integration algorithm.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1016/S0927-0256(03)00048-X
Chinese Library Classification Number:
Citation Information:
Considering the coupling effect between the nodal force equilibrium and internal variables evolution, an implicit scheme of solving the non-linear FEM problem is presented to modelling the texture evolution and the anisotropic behaviour of polycrystals for large deformation. This algorithm is based on the isomorphism theory that the current elastic law can be achieved through transferring the reference elastic law by a plastic transformation. Different time steps have been adopted with respect to the global and local iteration systems and the consistent tangent module is also calculated to construct a high speed integration algorithm.
quote
| GB/T 7714-2015 | [1] Anxin Ma. Computational Materials Science, 2003(27). DOI:10.1016/S0927-0256(03)00048-X. |
| MLA | [1] Anxin Ma. Computational Materials Science, no. 27, 2003, https://doi.org/10.1016/S0927-0256(03)00048-X. |
| APA | [1] Anxin Ma. (2003). Computational Materials Science(27). https://doi.org/10.1016/S0927-0256(03)00048-X |
| IEEE | [1] Anxin Ma, Computational Materials Science, no. 27, 2003, doi: 10.1016/S0927-0256(03)00048-X. |