Press-transferred carbon black nanoparticles for class-selective antioxidant electrochemical detection AITranslate

University of Teramo; University of Teramo;Institute of Materials Science of Madrid (CSIC);Institute of Materials Science of Madrid (CSIC); University of Teramo; University of Teramo; University of Teramo; University of Alcalá
AITranslate
Publisher: Elsevier
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Carbon black nanoparticles (CBNPs) press imprinted films are proposed for class-selective electrochemical detection of ortho-diphenols (o-diphenols) and mono-phenols (m-phenols) antioxidants. In order to optimize the sensor construction, different surface immobilizations of CBNPs electroactive films on a PMMA support were assayed by using different amounts of CBNPs dispersions. The best sensor in terms of selectivity, sensitivity and stability was obtained when 30 mL of a CBNPs dispersion (0.50 mg/100 mL in 1,2-dichloroethane) were transferred onto PMMA substrates applying a pressure of 4.6 ton. The electrodes were characterized by Electrochemical Impedance Spectroscopy (EIS) and Cyclic Voltammetry (CV) to explore their electrical properties. The effective transfer of CBNPs on the PMMA support and the CBNPs film conductivity have been evaluated by Atomic Force Microscopy (AFM) confirming that the carbon black film is effectively imprinted on the polymer surface and that retains its good conductivity. X-ray Photoelectron Spectroscopy (XPS) and Raman spectroscopy have been employed to investigate the CBNPs composition and the CBNPs electrode surface, respectively. CBNPs electrodes exclusively supported the o-diphenols and m-phenols sensing, at low detection potentials (+0.100 and +0.560 V, respectively) and with negligible surface fouling (peak intensity RSDs <12% and oxidation potential <6%, n = 28). Class-selective electrochemical indexes (EIs) for o-diphenols and m-phenols are proposed for the evaluation of the phenols antioxidant contents in complex samples such as olive oils. Graphical abstract Download : Download high-res image (102KB) Download : Download full-size image

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1016/j.apmt.2017.04.012

Chinese Library Classification Number:

Citation Information:

Carbon black nanoparticles (CBNPs) press imprinted films are proposed for class-selective electrochemical detection of ortho-diphenols (o-diphenols) and mono-phenols (m-phenols) antioxidants. In order to optimize the sensor construction, different surface immobilizations of CBNPs electroactive films on a PMMA support were assayed by using different amounts of CBNPs dispersions. The best sensor in terms of selectivity, sensitivity and stability was obtained when 30 mL of a CBNPs dispersion (0.50 mg/100 mL in 1,2-dichloroethane) were transferred onto PMMA substrates applying a pressure of 4.6 ton. The electrodes were characterized by Electrochemical Impedance Spectroscopy (EIS) and Cyclic Voltammetry (CV) to explore their electrical properties. The effective transfer of CBNPs on the PMMA support and the CBNPs film conductivity have been evaluated by Atomic Force Microscopy (AFM) confirming that the carbon black film is effectively imprinted on the polymer surface and that retains its good conductivity. X-ray Photoelectron Spectroscopy (XPS) and Raman spectroscopy have been employed to investigate the CBNPs composition and the CBNPs electrode surface, respectively. CBNPs electrodes exclusively supported the o-diphenols and m-phenols sensing, at low detection potentials (+0.100 and +0.560 V, respectively) and with negligible surface fouling (peak intensity RSDs <12% and oxidation potential <6%, n = 28). Class-selective electrochemical indexes (EIs) for o-diphenols and m-phenols are proposed for the evaluation of the phenols antioxidant contents in complex samples such as olive oils. Graphical abstract Download : Download high-res image (102KB) Download : Download full-size image

quote

GB/T 7714-2015 [1] Flavio Della Pelle, Roberto Di Battista, Luis Vázquez, et al. Applied Materials Today, 2017(9). DOI:10.1016/j.apmt.2017.04.012.
MLA [1] Flavio Della Pelle, et al., Applied Materials Today, no. 9, 2017, https://doi.org/10.1016/j.apmt.2017.04.012.
APA [1] Flavio Della Pelle, Roberto Di Battista, Luis Vázquez, F. Javier Palomares, Michele Del Carlo, Manuel Sergi, Dario Compagnone, & Alberto Escarpa. (2017). Applied Materials Today(9). https://doi.org/10.1016/j.apmt.2017.04.012
IEEE [1] Flavio Della Pelle, Roberto Di Battista, Luis Vázquez, F. Javier Palomares, Michele Del Carlo, Manuel Sergi, Dario Compagnone, and Alberto Escarpa, Applied Materials Today, no. 9, 2017, doi: 10.1016/j.apmt.2017.04.012.