daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Waterborne Poly(butylene succinate)-Coated Paper for Sustainable Packaging Applications AITranslate

Michigan State University; Michigan State University; Michigan State University; Michigan State University; Michigan State University; Michigan State University; Michigan State University; Michigan State University; Michigan State University; Michigan State University; Michigan State University; Michigan State University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Reported herein is waterborne poly(butylene succinate) (PBS)-coated paper as a potential biodegradable packaging material. Kraft paper was coated with PBS latex, and the coated paper was evaluated for its water and oil repellency, water vapor barrier performance, and physicomechanical properties. The water resistance (Cobb1800 value = 15.5 ± 0.1 g/m2), oil resistance (kit rating = 12/12), and water vapor transmission rate (112.62 ± 8.04 g/(m2 day) were observed for the coated paper. In addition, the coated paper showed excellent thermal sealing properties. Furthermore, a comparative performance study of our coated paper was performed against multiple commercial benchmarks. The PBS-latex-coated paper showed kit rating performance that matched or surpassed those of commercial benchmarks while having better water resistance than at least two tested commercial benchmarks. The biodegradation study in composting conditions indicates that the one-sided coated paper does not potentially affect the overall biodegradation of the coated paper.

KeyWords AITranslate

thermoplastic biodegradable waterresistant oilresistant thermal sealing
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.3c00846

Chinese Library Classification Number:

Citation Information:

Reported herein is waterborne poly(butylene succinate) (PBS)-coated paper as a potential biodegradable packaging material. Kraft paper was coated with PBS latex, and the coated paper was evaluated for its water and oil repellency, water vapor barrier performance, and physicomechanical properties. The water resistance (Cobb1800 value = 15.5 ± 0.1 g/m2), oil resistance (kit rating = 12/12), and water vapor transmission rate (112.62 ± 8.04 g/(m2 day) were observed for the coated paper. In addition, the coated paper showed excellent thermal sealing properties. Furthermore, a comparative performance study of our coated paper was performed against multiple commercial benchmarks. The PBS-latex-coated paper showed kit rating performance that matched or surpassed those of commercial benchmarks while having better water resistance than at least two tested commercial benchmarks. The biodegradation study in composting conditions indicates that the one-sided coated paper does not potentially affect the overall biodegradation of the coated paper.

quote

GB/T 7714-2015 [1] Syeda Shamila Hamdani, Hannah Emch, Jacob Isherwood, et al. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.3c00846.
MLA [1] Syeda Shamila Hamdani, et al., ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.3c00846.
APA [1] Syeda Shamila Hamdani, Hannah Emch, Jacob Isherwood, Ajmir Khan, Vikash Kumar, Alexandra Alford, Ian Wyman, Rishi Sharma, Pooja Mayekar, Anibal Bher, Rafael Auras, & Muhammad Rabnawaz. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.3c00846
IEEE [1] Syeda Shamila Hamdani, Hannah Emch, Jacob Isherwood, Ajmir Khan, Vikash Kumar, Alexandra Alford, Ian Wyman, Rishi Sharma, Pooja Mayekar, Anibal Bher, Rafael Auras, and Muhammad Rabnawaz, ACS Applied Polymer Materials, no. 5, 2023, doi: 10.1021/acsapm.3c00846. keywords: {thermoplastic;biodegradable;waterresistant;oilresistant;thermal sealing}