Electrode Separators for the Next-Generation Alkaline Water Electrolyzers AITranslate

Technical University of Denmark; Technical University of Denmark; Technical University of Denmark; Technical University of Denmark; Technical University of Denmark; University of Patras; University of Patras; Rensselaer Polytechnic Institute; Lund University; Korea University; Technical University of Denmark
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Multi-gigawatt-scale hydrogen production by water electrolysis is central in the green transition when it comes to storage of energy and forming the basis for sustainable fuels and materials. Alkaline water electrolysis plays a key role in this context, as the scale of implementation is not limited by the availability of scarce and expensive raw materials. Even though it is a mature technology, the new technological context of the renewable energy system demands more from the systems in terms of higher energy efficiency, enhanced rate capability, as well as dynamic, part-load, and differential pressure operation capability. New electrode separators that can support high currents at small ohmic losses, while effectively suppressing gas crossover, are essential to achieving this. This Focus Review compares the three main development paths that are currently being pursued in the field with the aim to identify the advantages and drawbacks of the different approaches in order to illuminate rational ways forward.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.3c00185

Chinese Library Classification Number:

Citation Information:

Multi-gigawatt-scale hydrogen production by water electrolysis is central in the green transition when it comes to storage of energy and forming the basis for sustainable fuels and materials. Alkaline water electrolysis plays a key role in this context, as the scale of implementation is not limited by the availability of scarce and expensive raw materials. Even though it is a mature technology, the new technological context of the renewable energy system demands more from the systems in terms of higher energy efficiency, enhanced rate capability, as well as dynamic, part-load, and differential pressure operation capability. New electrode separators that can support high currents at small ohmic losses, while effectively suppressing gas crossover, are essential to achieving this. This Focus Review compares the three main development paths that are currently being pursued in the field with the aim to identify the advantages and drawbacks of the different approaches in order to illuminate rational ways forward.

quote

GB/T 7714-2015 [1] David Aili, Mikkel Rykær Kraglund, Sinu C. Rajappan, et al. ACS Energy Letters, 2023(8). DOI:10.1021/acsenergylett.3c00185.
MLA [1] David Aili, et al., ACS Energy Letters, no. 8, 2023, https://doi.org/10.1021/acsenergylett.3c00185.
APA [1] David Aili, Mikkel Rykær Kraglund, Sinu C. Rajappan, Dmytro Serhiichuk, Yifan Xia, Valadoula Deimede, Joannis Kallitsis, Chulsung Bae, Patric Jannasch, Dirk Henkensmeier, & Jens Oluf Jensen. (2023). ACS Energy Letters(8). https://doi.org/10.1021/acsenergylett.3c00185
IEEE [1] David Aili, Mikkel Rykær Kraglund, Sinu C. Rajappan, Dmytro Serhiichuk, Yifan Xia, Valadoula Deimede, Joannis Kallitsis, Chulsung Bae, Patric Jannasch, Dirk Henkensmeier, and Jens Oluf Jensen, ACS Energy Letters, no. 8, 2023, doi: 10.1021/acsenergylett.3c00185.