Abstract AITranslate

It is of great interest to determine whether a relatively easily prepared and inexpensive protic ionic liquid (PIL) could be used in place of an aprotic ionic liquid (AIL) in a composite membrane for CO2 separation. We prepared mechanically reliable sulfonated polyimide (SPI) composite membranes with a PIL, [N124][NTf2] (N,N,N-butylethylmethylammonium bis(trifluoromethylsulfonyl)amide) by a solution casting method, and their mechanical, thermal, and gas separation (CO2 and N2) properties were compared with those of membranes incorporating an isomeric AIL, [N1123][NTf2] ([N1123]+, N,N,N,N-ethyldimethylpropylammonium). We discussed the influence of the presence or absence of active protons in the ILs on CO2 separation characteristics and the applicability of the PIL to a CO2 separation membrane. The SPI/PIL membrane exhibited a slightly lower selectivity, but higher permeability, than the SPI/AIL membrane. It is supposed that these differences originate from the difference in membrane structure and CO2 interactions between PIL and AIL, which was investigated through a combination of ab initio calculations, CO2 solubility measurements, and dynamic mechanical analysis. The [N124][NTf2](PIL)/SPI membranes showed a CO2 permeability (PCO2 = 240 Barrer) with a relatively high selectivity (αCO2/N2 = 23) at 30 °C, which indicates that a PIL/SPI composite membrane can be employed for CO2 separation. We also explored CO2 separation under elevated temperatures and humidified conditions for confirming the applicability of the SPI/PIL membrane. Finally, the effect of PIL structures was studied by using [N122][NTf2] ([N122]+, N,N,N-diethylmethylammonium) in comparison with [N124][NTf2]. Composite [N122][NTf2]/SPI membranes exhibited a comparable selectivity and an improved permeability. We anticipate these results will unveil a new paradigm in functional ion gels for critical CO2 separation technology, toward utilization of effective, benign materials.

KeyWords AITranslate

ionic liquid protic ionic liquid ion gel carbon dioxide separation membrane sulfonated polyimide
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.9b00383

Chinese Library Classification Number:

Citation Information:

It is of great interest to determine whether a relatively easily prepared and inexpensive protic ionic liquid (PIL) could be used in place of an aprotic ionic liquid (AIL) in a composite membrane for CO2 separation. We prepared mechanically reliable sulfonated polyimide (SPI) composite membranes with a PIL, [N124][NTf2] (N,N,N-butylethylmethylammonium bis(trifluoromethylsulfonyl)amide) by a solution casting method, and their mechanical, thermal, and gas separation (CO2 and N2) properties were compared with those of membranes incorporating an isomeric AIL, [N1123][NTf2] ([N1123]+, N,N,N,N-ethyldimethylpropylammonium). We discussed the influence of the presence or absence of active protons in the ILs on CO2 separation characteristics and the applicability of the PIL to a CO2 separation membrane. The SPI/PIL membrane exhibited a slightly lower selectivity, but higher permeability, than the SPI/AIL membrane. It is supposed that these differences originate from the difference in membrane structure and CO2 interactions between PIL and AIL, which was investigated through a combination of ab initio calculations, CO2 solubility measurements, and dynamic mechanical analysis. The [N124][NTf2](PIL)/SPI membranes showed a CO2 permeability (PCO2 = 240 Barrer) with a relatively high selectivity (αCO2/N2 = 23) at 30 °C, which indicates that a PIL/SPI composite membrane can be employed for CO2 separation. We also explored CO2 separation under elevated temperatures and humidified conditions for confirming the applicability of the SPI/PIL membrane. Finally, the effect of PIL structures was studied by using [N122][NTf2] ([N122]+, N,N,N-diethylmethylammonium) in comparison with [N124][NTf2]. Composite [N122][NTf2]/SPI membranes exhibited a comparable selectivity and an improved permeability. We anticipate these results will unveil a new paradigm in functional ion gels for critical CO2 separation technology, toward utilization of effective, benign materials.

quote

GB/T 7714-2015 [1] Eri Hayashi, Morgan L. Thomas, Kei Hashimoto, et al. ACS Applied Polymer Materials, 2019(1). DOI:10.1021/acsapm.9b00383.
MLA [1] Eri Hayashi, et al., ACS Applied Polymer Materials, no. 1, 2019, https://doi.org/10.1021/acsapm.9b00383.
APA [1] Eri Hayashi, Morgan L. Thomas, Kei Hashimoto, Seiji Tsuzuki, Akika Ito, & Masayoshi Watanabe. (2019). ACS Applied Polymer Materials(1). https://doi.org/10.1021/acsapm.9b00383
IEEE [1] Eri Hayashi, Morgan L. Thomas, Kei Hashimoto, Seiji Tsuzuki, Akika Ito, and Masayoshi Watanabe, ACS Applied Polymer Materials, no. 1, 2019, doi: 10.1021/acsapm.9b00383. keywords: {ionic liquid;protic ionic liquid;ion gel;carbon dioxide separation membrane;sulfonated polyimide}