Photothermal and Humidity Stimulus-Responsive Self-Sensing Soft Actuators for Smart Packaging AITranslate

Wuhan University; Wuhan University; Wuhan University; Wuhan University; Wuhan University; Wuhan University; Wuhan University; Wuhan University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Soft actuators with both actuation and self-sensing characteristics can better adapt to the environment and more effectively realize intelligent human–machine interactions, which is highly desired for the upcoming era of soft robotics. Herein, a multi-stimulus response actuator (MSRA) is constructed based on the asymmetric expansion principle, and the sensing function is simply and quickly integrated into the soft actuator by screen printing technology. Taking advantage of the good photothermal conversion performance of the dopamine-modified graphene oxide (DGO) layer and the difference in the expansion coefficient between the DGO layer and the poly(vinylidene fluoride)/polydimethylsiloxane layer, the soft actuators exhibit different actuation behaviors under photothermal and humidity stimuli, respectively. Meanwhile, the introduction of a printed carbon black/highly elastic transparent adhesive cement sensing layer gives MSRA a self-sensing function which can provide feedback on its actuation process in real time. In addition, various complex deformations can be achieved by the macroscopic assembly of several actuators. Finally, we show that this soft actuator can be used as a smart packaging material to realize smart packaging. We believe that actuators with sensing feedback are significant in soft robots and smart packaging.

KeyWords AITranslate

selfsensing soft actuator multistimulus response complex deformations soft robots smart packaging
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.3c00627

Chinese Library Classification Number:

Citation Information:

Soft actuators with both actuation and self-sensing characteristics can better adapt to the environment and more effectively realize intelligent human–machine interactions, which is highly desired for the upcoming era of soft robotics. Herein, a multi-stimulus response actuator (MSRA) is constructed based on the asymmetric expansion principle, and the sensing function is simply and quickly integrated into the soft actuator by screen printing technology. Taking advantage of the good photothermal conversion performance of the dopamine-modified graphene oxide (DGO) layer and the difference in the expansion coefficient between the DGO layer and the poly(vinylidene fluoride)/polydimethylsiloxane layer, the soft actuators exhibit different actuation behaviors under photothermal and humidity stimuli, respectively. Meanwhile, the introduction of a printed carbon black/highly elastic transparent adhesive cement sensing layer gives MSRA a self-sensing function which can provide feedback on its actuation process in real time. In addition, various complex deformations can be achieved by the macroscopic assembly of several actuators. Finally, we show that this soft actuator can be used as a smart packaging material to realize smart packaging. We believe that actuators with sensing feedback are significant in soft robots and smart packaging.

quote

GB/T 7714-2015 [1] Enbo Xue, Bin Tian, Youfusheng Wu, et al. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.3c00627.
MLA [1] Enbo Xue, et al., ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.3c00627.
APA [1] Enbo Xue, Bin Tian, Youfusheng Wu, Qun Liu, Panwang Guo, Ke Zheng, Jing Liang, & Wei Wu. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.3c00627
IEEE [1] Enbo Xue, Bin Tian, Youfusheng Wu, Qun Liu, Panwang Guo, Ke Zheng, Jing Liang, and Wei Wu, ACS Applied Polymer Materials, no. 5, 2023, doi: 10.1021/acsapm.3c00627. keywords: {selfsensing soft actuator;multistimulus response;complex deformations;soft robots;smart packaging}