Impacts of Imidazolate Ligand on Performance of Zeolitic-Imidazolate Framework-Derived Oxygen Reduction Catalysts AITranslate
Abstract AITranslate
Carbon-hosted Fe–N-coordinated (Fe/N/C) materials, especially those derived from thermolysis of iron-added zinc-based zeolite-imidazolate frameworks (ZIFs), have emerged as the most promising platinum group metal-free (PGM-free) oxygen reduction reaction (ORR) catalysts. However, the impacts of the precursory ZIF structure and their conversion chemistry during thermal activation to the final catalytic activity remain to be further explored in the process of continuously refining the catalyst performance. Herein, we synthesized a series of Fe-doped ZIFs with different imidazolate ligands and systematically studied the correlation between the crystal structures with the final ORR catalytic activity in an alkaline electrolyte. We also investigated the ZIF decomposition chemistry during pyrolysis using a thermogravimetric mass-spectroscopic analysis. We demonstrated that imidazole side-chain substitution alters the ZIF’s decomposition during pyrolysis, influencing the elemental compositions, surface properties, graphitization levels, and ultimately the catalytic performance. The Zn(mIm)2TPIBP catalyst affords the highest ORR activity with a half-wave potential of 0.93 V vs RHE, representing the best among all PGM-free catalysts studied.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsenergylett.9b01740
Chinese Library Classification Number:
Citation Information:
Carbon-hosted Fe–N-coordinated (Fe/N/C) materials, especially those derived from thermolysis of iron-added zinc-based zeolite-imidazolate frameworks (ZIFs), have emerged as the most promising platinum group metal-free (PGM-free) oxygen reduction reaction (ORR) catalysts. However, the impacts of the precursory ZIF structure and their conversion chemistry during thermal activation to the final catalytic activity remain to be further explored in the process of continuously refining the catalyst performance. Herein, we synthesized a series of Fe-doped ZIFs with different imidazolate ligands and systematically studied the correlation between the crystal structures with the final ORR catalytic activity in an alkaline electrolyte. We also investigated the ZIF decomposition chemistry during pyrolysis using a thermogravimetric mass-spectroscopic analysis. We demonstrated that imidazole side-chain substitution alters the ZIF’s decomposition during pyrolysis, influencing the elemental compositions, surface properties, graphitization levels, and ultimately the catalytic performance. The Zn(mIm)2TPIBP catalyst affords the highest ORR activity with a half-wave potential of 0.93 V vs RHE, representing the best among all PGM-free catalysts studied.
quote
| GB/T 7714-2015 | [1] Hao Wang, Lauren R. Grabstanowicz, Heather M. Barkholtz, et al. ACS Energy Letters, 2019(4). DOI:10.1021/acsenergylett.9b01740. |
| MLA | [1] Hao Wang, et al., ACS Energy Letters, no. 4, 2019, https://doi.org/10.1021/acsenergylett.9b01740. |
| APA | [1] Hao Wang, Lauren R. Grabstanowicz, Heather M. Barkholtz, Dominic Rebollar, Zachary B. Kaiser, Dan Zhao, BiaoHua Chen, & DiJia Liu. (2019). ACS Energy Letters(4). https://doi.org/10.1021/acsenergylett.9b01740 |
| IEEE | [1] Hao Wang, Lauren R. Grabstanowicz, Heather M. Barkholtz, Dominic Rebollar, Zachary B. Kaiser, Dan Zhao, BiaoHua Chen, and DiJia Liu, ACS Energy Letters, no. 4, 2019, doi: 10.1021/acsenergylett.9b01740. |