daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Recyclable Ionic Conductive Hydrogels Based on Autonomous Polymerization of α-Lipoic Acid for Flexible Wearable Electronic Sensors AITranslate

Qilu University of Technology (Shandong Academy of Sciences); Qilu University of Technology (Shandong Academy of Sciences); Qilu University of Technology (Shandong Academy of Sciences);Kyiv National University of Technologies and Design; Qilu University of Technology (Shandong Academy of Sciences); Qilu University of Technology (Shandong Academy of Sciences)
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Ionic conductive hydrogels (ICHs) have attracted extensive attention in the field of flexible wearable electronic sensors as a result of softness, biocompatibility, self-healing ability, mechanical elasticity, and high-sensitivity conductivity. However, the existing preparation process of ICHs is mostly complicated, and the use of nonrenewable raw materials might be unfavorable for the recycling of ICHs. Therefore, taking into account extensibility, ion conductivity, self-healing, and adhesion, how to prepare ICHs with excellent recyclability by a simple and practicable method remains a great challenge. In this work, poly(α-lipoic acid) (PLA), Fe3+, sodium alginate (SA), and 1-ethyl-3-methylimidazolium ethyl sulfate ([EMI][ES]) are used to achieve the above functions of ICHs. Because of the reversibility of dynamic interactions (including metal coordination bonds, ionic bonds, hydrogen bonds, and electrostatic interactions), the prepared ICHs have remarkable stretchability (2000%), self-healing property (96.37% efficiency), and adhesiveness. In addition, the conductivity sensitivity (GF) of the ICH can reach 1.31, and the response time can improve to 205 ms. As a flexible wearable electronic sensor, it can monitor and distinguish large-scale human movements and subtle physiological activities. Moreover, the ICH can be completely recovered and reused through simply dissolving with water and solvent evaporation without a significant loss of original functions. This ionic conductive hydrogel with synergistic functions is expected to provide a way for people to develop ideal green flexible wearable electronic sensors.

KeyWords AITranslate

ionic conductive hydrogels selfhealing reusability high sensitivity high adhesion strain sensor
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.3c01567

Chinese Library Classification Number:

Citation Information:

Ionic conductive hydrogels (ICHs) have attracted extensive attention in the field of flexible wearable electronic sensors as a result of softness, biocompatibility, self-healing ability, mechanical elasticity, and high-sensitivity conductivity. However, the existing preparation process of ICHs is mostly complicated, and the use of nonrenewable raw materials might be unfavorable for the recycling of ICHs. Therefore, taking into account extensibility, ion conductivity, self-healing, and adhesion, how to prepare ICHs with excellent recyclability by a simple and practicable method remains a great challenge. In this work, poly(α-lipoic acid) (PLA), Fe3+, sodium alginate (SA), and 1-ethyl-3-methylimidazolium ethyl sulfate ([EMI][ES]) are used to achieve the above functions of ICHs. Because of the reversibility of dynamic interactions (including metal coordination bonds, ionic bonds, hydrogen bonds, and electrostatic interactions), the prepared ICHs have remarkable stretchability (2000%), self-healing property (96.37% efficiency), and adhesiveness. In addition, the conductivity sensitivity (GF) of the ICH can reach 1.31, and the response time can improve to 205 ms. As a flexible wearable electronic sensor, it can monitor and distinguish large-scale human movements and subtle physiological activities. Moreover, the ICH can be completely recovered and reused through simply dissolving with water and solvent evaporation without a significant loss of original functions. This ionic conductive hydrogel with synergistic functions is expected to provide a way for people to develop ideal green flexible wearable electronic sensors.

quote

GB/T 7714-2015 [1] Yunxiang Fan, Xin Wang, Xujing Zhang, et al. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.3c01567.
MLA [1] Yunxiang Fan, et al., ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.3c01567.
APA [1] Yunxiang Fan, Xin Wang, Xujing Zhang, Zhihao Chang, Wei Kuang, & Huilin Tian. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.3c01567
IEEE [1] Yunxiang Fan, Xin Wang, Xujing Zhang, Zhihao Chang, Wei Kuang, and Huilin Tian, ACS Applied Polymer Materials, no. 5, 2023, doi: 10.1021/acsapm.3c01567. keywords: {ionic conductive hydrogels;selfhealing;reusability;high sensitivity;high adhesion;strain sensor}