Shape-memory epoxy resin (SMER) with strong mechanical properties have potential for a wide range of applications, but the design and synthesis of SMER with both high mechanical property and short shape recovery time are still a challenge. Hyperbranched epoxy resin shape-memory materials offer a unique approach that has been investigated by very few researchers because of the tedious synthetic process. In this work, serial hyperbranched epoxy resins with different molecular weights and structures (ETMP-n, ETHP-n, n = 6, 9, 11) were synthesized by a simple highly efficient thiol-maleimide click reaction. Cured ETHP-n films display shape fixity ratios and shape recovery ratios as high as 98.5% and 97.2% after seven shape-memory cycles, respectively. Cured ETMP-9 and ETHP-9 films demonstrate rapid response, with shape recovery times as short as 450 and 430 ms, respectively, which are significantly shorter than previously reported shape-memory epoxy resins. The maximum actuated stress of cured films reaches 0.72 MPa, which was much higher than that of most mammalian skeletal muscles (0.35 MPa). Cured ETHP-9 films exhibited higher shape-memory performances than cured ETMP-9 films because of nitrogen heterocyclic rigid structures, appropriately high cross-link density and narrower molecular weight distribution. These excellent shape-memory performances make the hyperbranched epoxy resins suitable for practical applications in microelectronic devices and artificial muscles.

KeyWords AITranslate

hyperbranched epoxy resins thiolmaleimide click reaction shape memory rapid response high mechanical strength
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.2c00625

Chinese Library Classification Number:

Citation Information:

Shape-memory epoxy resin (SMER) with strong mechanical properties have potential for a wide range of applications, but the design and synthesis of SMER with both high mechanical property and short shape recovery time are still a challenge. Hyperbranched epoxy resin shape-memory materials offer a unique approach that has been investigated by very few researchers because of the tedious synthetic process. In this work, serial hyperbranched epoxy resins with different molecular weights and structures (ETMP-n, ETHP-n, n = 6, 9, 11) were synthesized by a simple highly efficient thiol-maleimide click reaction. Cured ETHP-n films display shape fixity ratios and shape recovery ratios as high as 98.5% and 97.2% after seven shape-memory cycles, respectively. Cured ETMP-9 and ETHP-9 films demonstrate rapid response, with shape recovery times as short as 450 and 430 ms, respectively, which are significantly shorter than previously reported shape-memory epoxy resins. The maximum actuated stress of cured films reaches 0.72 MPa, which was much higher than that of most mammalian skeletal muscles (0.35 MPa). Cured ETHP-9 films exhibited higher shape-memory performances than cured ETMP-9 films because of nitrogen heterocyclic rigid structures, appropriately high cross-link density and narrower molecular weight distribution. These excellent shape-memory performances make the hyperbranched epoxy resins suitable for practical applications in microelectronic devices and artificial muscles.

quote

GB/T 7714-2015 [1] Yanfen Lu, Haifeng Xu, Nuo Liang, et al. ACS Applied Polymer Materials, 2022(4). DOI:10.1021/acsapm.2c00625.
MLA [1] Yanfen Lu, et al., ACS Applied Polymer Materials, no. 4, 2022, https://doi.org/10.1021/acsapm.2c00625.
APA [1] Yanfen Lu, Haifeng Xu, Nuo Liang, Zejun Xu, Sufang Chen, & Daohong Zhang. (2022). ACS Applied Polymer Materials(4). https://doi.org/10.1021/acsapm.2c00625
IEEE [1] Yanfen Lu, Haifeng Xu, Nuo Liang, Zejun Xu, Sufang Chen, and Daohong Zhang, ACS Applied Polymer Materials, no. 4, 2022, doi: 10.1021/acsapm.2c00625. keywords: {hyperbranched epoxy resins;thiolmaleimide;click reaction;shape memory;rapid response;high mechanical strength}