daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

A crystal plasticity study of the effect of friction on the evolution of texture and mechanical behaviour in the nano-indentation of an aluminium single crystal AITranslate

University of Wollongong; University of Wollongong; University of Wollongong; University of Wollongong; University of Wollongong
AITranslate
Publisher: Elsevier
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Highlights • COF almost does not affect the load–displacement curves. • Young’s modulus decreases with the increasing COF. • Influence of COF on the indentation hardness is very small. • Lattice rotation is dependent with the COF. A crystal plasticity finite element method (CPFEM) model has been developed to investigate the effect of the coefficient of friction (COF) on the evolution of crystallographic texture and mechanical behaviour of the initially oriented aluminium single crystal during nano-indentation. The simulation results have been validated by comparing with the experimental observations. The load–displacement curves from the simulation with different COFs have been analysed and the calculated values of Young’s moduli agree well with the real material. The indentation hardness with different COFs has been investigated and the deviation is quite small. The piling-up curve was captured on the deformed surface and it decreased when the COF increased. Sinking-in curve was also captured and it increased when the COF increased. The pole figures and the lattice rotation angles after unloading were calculated and then analysed. The analysis revealed that these lattice rotation angles in the chosen deformed zone were significantly affected by the COF during nano-indentation.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1016/j.commatsci.2013.05.030

Chinese Library Classification Number:

Citation Information:

Highlights • COF almost does not affect the load–displacement curves. • Young’s modulus decreases with the increasing COF. • Influence of COF on the indentation hardness is very small. • Lattice rotation is dependent with the COF. A crystal plasticity finite element method (CPFEM) model has been developed to investigate the effect of the coefficient of friction (COF) on the evolution of crystallographic texture and mechanical behaviour of the initially oriented aluminium single crystal during nano-indentation. The simulation results have been validated by comparing with the experimental observations. The load–displacement curves from the simulation with different COFs have been analysed and the calculated values of Young’s moduli agree well with the real material. The indentation hardness with different COFs has been investigated and the deviation is quite small. The piling-up curve was captured on the deformed surface and it decreased when the COF increased. Sinking-in curve was also captured and it increased when the COF increased. The pole figures and the lattice rotation angles after unloading were calculated and then analysed. The analysis revealed that these lattice rotation angles in the chosen deformed zone were significantly affected by the COF during nano-indentation.

quote

GB/T 7714-2015 [1] Mao Liu, Anh Kiet Tieu, Cheng Lu, et al. Computational Materials Science, 2014(81). DOI:10.1016/j.commatsci.2013.05.030.
MLA [1] Mao Liu, et al., Computational Materials Science, no. 81, 2014, https://doi.org/10.1016/j.commatsci.2013.05.030.
APA [1] Mao Liu, Anh Kiet Tieu, Cheng Lu, Hongtao Zhu, & Guanyu Deng. (2014). Computational Materials Science(81). https://doi.org/10.1016/j.commatsci.2013.05.030
IEEE [1] Mao Liu, Anh Kiet Tieu, Cheng Lu, Hongtao Zhu, and Guanyu Deng, Computational Materials Science, no. 81, 2014, doi: 10.1016/j.commatsci.2013.05.030.